MP 55305

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MP 55305

Main features

  • No-Prep Impact-Resistant Bonding
  • 2 to 3-Minute Open Time
  • Thermal-Cycling and Chemical Resistance

Product Description

MP-55305 is a high-performance, two-part structural methyl methacrylate (MMA) adhesive designed for bonding a wide range of materials, including plastics, metals, and composites. It cures at room temperature and delivers exceptional strength and stiffness with outstanding resistance to temperature fluctuations, thermal cycling, and harsh chemicals without requiring surface preparation.

Key features

  • No surface preparation required: Ensures long-lasting reliability and high impact resistance without the need to prepare most surfaces.
  • Fast curing and convenient: Features a 1:1 mix ratio with a 2 to 3 minute open time and achieves fixture in 5 to 8 minutes at room temperature.
  • UL Certified: Recognized as a component for sign accessories under file number E350958.

Applications / Suitable for

  • Suitable for bonding metals such as aluminum, steel, stainless steel, and e-coated metal.
  • Designed for thermosets including fiberglass, phenolic, epoxy, and polyurethane.
  • Ideal for thermoplastics like acrylic, ABS, polycarbonate, PVC, and nylon/PA.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber or green, viscous liquid
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
2–3 min minutes
Product Type
Material category or functional product class.
Two-part modified acrylic structural adhesive

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure properties of MP-55305 structural adhesive.

Property Value Unit Method / condition
Appearance / Color Amber or Green - -
Mix Ratio (Volume & Weight) 1:1 - -
Viscosity (Resin) 60,000-80,000 cPs Brookfield RV7, 20 RPM, 25°C
Viscosity (Activator) 60,000-120,000 cPs Brookfield RV7, 20 RPM, 25°C
Mixed Density 0.98 g/cc -
Open Time 2-3 Minutes -
Fixture Time 5-8 Minutes -

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers