MP 54110

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

MP 54110 MP 54110

Main features

  • 1:1 Meter-Mix Dispensing
  • 30-60 Minute Handling Cure
  • 15.9 MPa Aluminum Shear

Product Description

H.B. Fuller MP54110 Epoxy Adhesive uses a clear, two-part unfilled epoxy system to bond metals, ceramics, and most plastics. The liquid components mix 1:1 by weight or volume and produce a typical mixed viscosity of 20,000 cP for cartridge and meter-mix-dispense application. At 25 deg C, a 20 g batch has an 8-12 minute pot life. Assemblies reach handling cure in 30-60 minutes and full cure in 24 hours at room temperature. The cured adhesive has Shore D 80 hardness, 10% elongation, and a typical operating range of -40 to 130 deg C.

Key features

  • One-to-one mix ratio: Mixes 1:1 by weight or volume for cartridge or meter-mix-dispense application.
  • Rapid handling cure: Reaches handling cure in 30-60 minutes at room temperature.
  • Aluminum overlap shear: Provides 15.9 MPa typical overlap shear on acid-etched aluminum under ASTM D1002 conditions.

Applications / Suitable for

  • Bonding metal and ceramic assemblies
  • Bonding most plastic assemblies
  • Cartridge or meter-mix-dispense application
Product Family

MP 54110

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Chemistry Type
Epoxy
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
two component

Additional Information

Technical properties

Uncured and working properties

Property Value Unit Method / condition
Appearance Clear liquid As supplied
Mix ratio 1:1 by weight or volume Resin to hardener
Mixed viscosity 20,000 cP Typical
Mixed specific gravity 1.16 Typical
Pot life 8-12 min 20 g mass at 25 deg C
Storage temperature 12-25 deg C Unopened containers
Technical properties

Cured properties

Property Value Unit Method / condition
Shore hardness 80 Shore D ASTM D2240
Operating temperature -40 to 130 deg C Typical range
Overlap shear 15.9 MPa ASTM D1002; acid-etched aluminum; 25 deg C; 50% RH
Elongation 10 % Cured adhesive