MP 5405

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

MP 5405

Main features

  • Multi-Substrate Structural Adhesion
  • Documented Water/Salt-Spray/Acid/Solvent Resistance
  • 3 to 5-Minute Handling Time

Product Description

MP5405 is a clear, two-part unfilled epoxy structural adhesive designed for bonding ceramics, metals, and most plastics. It features a 1:1 mix ratio and cures at room temperature to form a tough, semi-rigid material that offers strong resistance to water, salt spray, and various chemicals.

Key features

  • Fast handling strength: Achieves handling strength in 3 to 5 minutes at room temperature for quick assembly.
  • Excellent chemical resistance: Withstands water, salt spray, inorganic acids and bases, and most organic solvents.
  • Convenient 1:1 mix ratio: Easily dispensed using either static mixing nozzles in dual cartridges or MMD equipment.

Applications / Suitable for

  • Designed for bonding ceramics, metals, and most plastics.
  • Suitable for use in either MMD equipment or side-by-side dual cartridges.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear, free-flowing liquid
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
3–5 min minutes
Product Type
Material category or functional product class.
Two-part epoxy structural adhesive

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure properties of MP5405 epoxy adhesive.

Property Value Unit Method / condition
Appearance / Color Clear - -
Mix Ratio (Volume & Weight) 1:1 - -
Viscosity (Mixed) 12,500 cPs at 25°C
Specific Gravity (Mixed) 1.16 - -
Pot Life 3 to 5 min at 25°C, 20 gram
Technical properties

After-processing / final-state properties

Cured mechanical and electrical properties of MP5405 after full cure.

Property Value Unit Method / condition
Hardness 80 Shore D ASTM D2240
Tensile Strength 48.3 (7000) MPa (psi) ASTM D638
Overlap Shear Strength 15.9 (2300) MPa (psi) Aluminum, Acid Etched, 25°C, ASTM D1002
Operating Temperature -40 to 130 °C -
Dielectric Strength 16.1 kV/mm ASTM D149