MOLYKOTE PG54

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE PG54

Main features

  • Long-Term Lubrication for Metal-to-Plastic
  • 50 to 180 deg C Service Range
  • Silicone Base Oil

Product Description

MOLYKOTE® PG-54 Plastislip Grease is a white, silicone-oil-based grease developed for long-term lubrication of metal-to-plastic, plastic-to-plastic, and reinforced-rubber contact combinations. The NLGI Grade 2–3 formulation uses a lithium-complex thickener and PTFE solid lubricant to support low-friction movement, corrosion protection, and operation from −50°C to 180°C. It is suitable for bushings, gears, chains, sealing rings, sliding tracks, switches, and flexible control cables used in automotive systems, electric motors, gearboxes, and household or garden equipment.

Key features

  • Plastic and rubber compatibility: Intended for long-term lubrication of plastic, reinforced-rubber, and mixed metal-to-plastic contacts.
  • Wide operating-temperature range: Supports service from −50°C to 180°C.
  • Low-friction operation: Formulated for moving rubber and plastic components requiring controlled sliding behavior.
  • Corrosion protection: Provides supplier-documented corrosion protection for lubricated components.
  • Silicone-based formulation: Uses silicone base oil with a lithium-complex thickener.
  • Long-term lubrication: Suitable for extended lubrication of supported material combinations under appropriate service conditions.

Applications / Suitable for

  • Plastic and reinforced-rubber bearing bushings
  • Plastic gears and chains
  • Sealing rings, switches, sliding tracks, and guides
  • Flexible control cables and Bowden cable systems
  • Electric motors and gearboxes
  • Automotive brake and clutch systems

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Plastic-compatible grease; NLGI 2–3
Thermal Properties
Operating Temperature
−50°C to 180°C °C

Additional Information

Technical properties

As-supplied / before-processing properties

Supplier-published as-supplied characteristics of MOLYKOTE® PG-54 Plastislip Grease.

Property Value Unit Method / condition
Product type Grease — MOLYKOTE® grease classification
Base-oil technology Silicone — Supplier-listed technology
Thickener Lithium complex — Supplier-listed composition
Solid lubricant PTFE — Supplier-listed composition
Color White — As supplied
NLGI grade 2–3 — Consistency classification
Base-oil viscosity Approximately 200 cSt At 40°C
Technical properties

After-application / in-service properties

Supplier-documented operating characteristics relevant to the installed grease layer.

Property Value Unit Method / condition
Operating-temperature range −50 to 180 °C Supplier-listed operating range
Plastic and rubber compatibility Good — Supplier-documented qualitative characteristic
Coefficient-of-friction characteristic Low — Qualitative supplier claim; no numerical test value published on the accessible page
Corrosion protection Good — Supplier-documented qualitative characteristic
Lubrication duration Long-term lubrication — Application-dependent; no universal relubrication interval stated