MOLYKOTE P37

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE P37

Main features

  • -30 to 1400 deg C Threaded-Connection Lubrication
  • 5,500 N Four-Ball Weld Load
  • Graphite/Zirconium-Dioxide High-Purity Paste

Product Description

MOLYKOTE® P-37 Antiseize Paste is a gray-black, mineral-oil-based solid-lubricant paste for high-temperature bolted joints. Formulated with graphite and zirconium dioxide, it provides load-carrying capability and seizure protection for screws, nuts, and bolts made from heat-resistant and extremely heat-resistant steels, including nickel-based alloys. The paste supports assembly and later dismantling of threaded connections exposed to prolonged high temperatures and has been used on gas- and steam-turbine bolted joints in power stations. Its solid-lubricant system is temperature resistant from −30°C to 1,400°C, while low sulfur and total-halogen limits support use where lubricant purity is important.

Key features

  • Extreme-temperature capability: The solid-lubricant system is temperature resistant from −30°C to 1,400°C.
  • Seizure protection: Helps prevent seizure and supports removal of threaded fasteners after extended high-temperature exposure.
  • High load-carrying performance: Provides a typical four-ball weld load of 5,500 N.
  • High-purity formulation: Limits sulfur to 250 ppm maximum and total halogens, including chlorine, to 200 ppm maximum.
  • Low seepage: Suitable for applications where cleanliness around the lubricated connection is important.
  • High-temperature material stability: Does not include components identified by the supplier as becoming brittle at elevated temperatures.

Applications / Suitable for

  • High-temperature screws, nuts, and bolts
  • Threaded connections made from heat-resistant steels
  • Nickel-alloy fasteners and other extremely heat-resistant alloys
  • Gas-turbine bolted joints
  • Steam-turbine bolted joints
  • Power-generation assembly and maintenance operations

Technical Specifications

General Properties
Product Type
Material category or functional product class.
High-temperature anti-seize paste; NLGI 1–2
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.21 g/cm³ at 20°C
Thermal Properties
Operating Temperature
−30°C to 1,400°C for the solid-lubricant system °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for MOLYKOTE® P-37 Antiseize Paste. Values are not intended as specification limits.

Property Value Unit Method / condition
Product type Anti-seize solid-lubricant paste — For high-temperature threaded connections
Base-oil technology Mineral oil — Supplier-listed composition
Solid lubricants Graphite and zirconium dioxide — Current DuPont product details
Appearance Gray-black — Typical property
NLGI grade 1–2 — Supplier product classification
Unworked penetration 280–310 0.1 mm ISO 2137
Density 1.21 g/cm³ ISO 2811 at 20°C
Total halogen content ≤200 ppm Maximum; includes chlorine
Sulfur content ≤250 ppm Maximum
Usable life 60 months Original unopened container stored from 0°C to 35°C
Technical properties

After-application / in-service properties

Typical performance characteristics of the applied paste under the stated laboratory and bolted-joint test conditions.

Property Value Unit Method / condition
Solid-lubricant temperature resistance −30 to 1,400 °C Temperature resistance of the solid-lubricant system
Four-ball weld load 5,500 N DIN 51350-4; 1,450 rpm for 1 minute
Four-ball wear scar 1.50 mm DIN 51350-5; 1,450 rpm, 800 N, 1 hour
Thread coefficient of friction 0.11 μ M12 × 1.75, property class 8.8, blackened
Under-head coefficient of friction 0.11 μ M12 × 1.75, property class 8.8, blackened
Tightening torque 49.4 N·m 21CrMoNiV57 bolts; 600°C for 21 hours
Breakaway torque 120.9 N·m 21CrMoNiV57 bolts; 600°C for 21 hours
Tightening torque 49.4 N·m Nimonic NiCr20TiAl fasteners; 850°C for 4 weeks
Breakaway torque 102.4 N·m Nimonic NiCr20TiAl fasteners; 850°C for 4 weeks