MOLYKOTE P-40

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE P-40

Main features

  • Metal-Free Lubrication Paste
  • Assembly and Continuous Lubrication
  • -40 to 121 deg C Paste Service

Product Description

MOLYKOTE® P-40 (S) Paste is a metal-free adhesive lubrication paste for assembly and continuous lubrication, particularly where components are exposed to corrosive environments such as splash water or humidity. It combines adhesion with documented corrosion protection, water resistance, and anti-fretting characteristics. The paste has a service temperature range of -40 to +121°C (-40 to +250°F), while its solid lubricants are documented for -40 to +1,093°C (-40 to +2,000°F). Typical uses include threaded connections, spline shafts, bearing mounting, brake-system components, commercial-vehicle axles, cams, plain bearings, open gears, and marine applications.

Key features

  • Corrosive-environment lubrication: Provides documented corrosion protection and water resistance for applications exposed to splash water or humidity.
  • Assembly and continuous lubrication: Supports both assembly lubrication and continuous lubrication across a range of mechanical components.
  • Broad temperature capability: Paste service range is -40 to +121°C, with solid lubricants documented from -40 to +1,093°C.

Applications / Suitable for

  • Assembly and threaded connections, spline shafts, and bearing mounting
  • Brake-system components, brake rods, guide bolts, commercial-vehicle axles, cams, and plain bearings
  • Open gears and marine applications

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Anti-seize, assembly and continuous-lubrication paste; NLGI 1
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Current official density not verified
Thermal Properties
Operating Temperature
−40°C to 1,093°C; upper value applies to the solid-lubricant system °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties of MOLYKOTE® P-40 (S) Paste. Typical values are not intended as product specifications.

Property Value Unit Method / condition
Color Yellowish brown - Typical
Unworked penetration 310-350 mm/10 ISO 2137
Base oil viscosity 400 mm²/s DIN 51 562; at 40°C (104°F)
Usable life 60 months Original unopened container; stored between 0 and 40°C (32 to 104°F); from date of production
Technical properties

After-processing / final-state properties

Typical in-service and performance properties. Test results are method-specific and should not be interpreted as universal equipment limits.

Property Value Unit Method / condition
Service temperature range - as paste -40 to +121 °C Equivalent to -40 to +250°F
Service temperature range - solid lubricants -40 to +1,093 °C Equivalent to -40 to +2,000°F; applies specifically to solid lubricants
Weld load 3,600 N DIN 51 350 pt.4; four-ball tester (VKA)
Wear scar 0.72 mm DIN 51 350 pt.5; under 800 N load
Coefficient of friction - thread 0.13 µ Screw test; M12 x 1.75, material 8.8, blackened
Corrosion protection 0 degree of corrosion DIN 51 802; SKF-Emcor method