MOLYKOTE 1000

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 1000

Main features

  • No Intentional PFAS, Lead, or Nickel
  • -30 to 650 deg C Service Range
  • Consistent Friction and High Load Capacity

Product Description

MOLYKOTE® 1000 Paste is a lead-free, nickel-free, and PFAS-free anti-seize paste designed to optimize friction and reduce wear in threaded fasteners and metal-to-metal joints. Formulated with solid lubricants, powdered metals (including copper and zinc), and mineral oil, it ensures nondestructive dismantling of components even after prolonged exposure to high temperatures up to 650°C (1,202°F). It is heavily relied upon in demanding industrial environments to maintain constant pre-stressing forces through uniform friction coefficients.

Key features

  • High-temperature stability: Maintains robust anti-seize performance over a wide service temperature range of -30°C to 650°C (-22°F to 1,202°F).
  • Consistent friction and dismantling: Delivers an unchanged coefficient of friction even after multiple bolt retightening and loosening processes, allowing for reliable, nondestructive disassembly.
  • High load capacity & corrosion protection: Provides strong corrosion protection and withstands extreme pressures, featuring a four-ball weld load of 4,800 N.

Applications / Suitable for

  • Bolted joints subjected to high temperatures and corrosive environments that require eventual retightening or disconnection
  • Cylinder head bolts and nozzle head screws in plastic injection molding machines
  • Tension rings of centrifuges and heavily loaded threaded connections in the chemical industry

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Brown
Density (g)
1.26 g/cm3
Thermal Properties
Service temperature
-30 to 650 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Mineral oil, solid lubricants, thickener, powdered metal - Contains copper flakes and zinc powder
Physical State / Appearance Brown - Paste
Unworked Penetration 280-310 mm/10 ISO 2137
Density 1.26 g/ml at 20°C (68°F) (ISO 2811)
Usable Life (Paste) 60 months Stored at or below 20°C (68°F) in unopened containers
Usable Life (Aerosol) 24 months Stored between 5°C and 35°C in unopened containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -30 to 650 °C (-22 to 1,202 °F) Temperature resistance of solid lubricants
Four-Ball Tester Weld Load 4,800 N DIN 51 350 pt.4
Four-Ball Wear Scar 0.65 mm Under 400 N load (DIN 51 350 pt.5)
Almen-Wieland OK Load 20,000 N -
Almen-Wieland Frictional Force 2,600 N -
Coefficient of Friction (Thread) 0.13 - Screw test (M12, 8.8, blackened surface)
Coefficient of Friction (Head) 0.08 - Screw test (M12, 8.8, blackened surface)
Initial Break-Away Torque 135 Nm M12, starting torque 62 Nm, heat treatment at 540°C for 21 hr (bolt material 1.7709)
Corrosion Protection 1 - SKF-Emcor method (DIN 51 802)