LORD P-1292

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LORD P-1292

Main features

  • Platinum-Cure RTV Adhesion Promotion
  • Broad-Substrate Addition-Cure Silicone Adhesion
  • Hydrolytically Stable Silicone Bonding

Product Description

LORD® P-1292 Primer is a solvent-based primer designed for electronics applications to improve the adhesion of platinum-catalyzed RTV silicone rubbers to most metals and glass. It is formulated for use with addition-cure silicone systems, providing enhanced adhesion and superior hydrolytic stability for demanding bonding applications.

Key Features

  • Designed to bond platinum-catalyzed RTV silicone rubbers to most metals and glass.
  • Provides good adhesion on most substrates when used with addition-cured silicones.
  • Delivers superior hydrolytic stability for durable bonded assemblies.
  • Low-viscosity liquid suitable for brush or spray application.
  • Forms a chalky primer film after air drying prior to silicone application.

Suitable For

  • Electronics assembly applications
  • Bonding platinum-catalyzed RTV silicone rubbers to metal substrates
  • Bonding platinum-catalyzed RTV silicone rubbers to glass substrates
  • Surface preparation before application of addition-cure silicone materials

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Blue Liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.81
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
5 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
36 °C

Additional Information

As-Supplied / Before-Processing Properties

Property Value
Appearance Blue Liquid
Viscosity 5 cP @ 25°C
Specific Gravity 0.81 @ 25°C
Flash Point 36°C
Recommended Film Thickness 12.7–25.4 µm
Drying Time Air dry 30–60 minutes before applying silicone RTV
Shelf Life 1 year in original unopened container stored at 15–35°C

After-Processing / Final-State Properties

Property Value
Primer Film Appearance Chalky film after air drying

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers