Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 852/25GB

Main features

  • Welding/Fastener Replacement Bonding
  • 20 to 25-Minute Working Time
  • Prepared/Unprepared Metal/FRP/Plastic Bonding

Product Description

LORD® 852S/25GB Toughened Structural Acrylic Adhesive is a two-component structural acrylic adhesive system consisting of LORD® 852S Adhesive and LORD® Accelerator 25GB. It is designed to replace welding, brazing, riveting and other mechanical fastening methods while providing structural bonding of prepared and unprepared metals, polymer composite substrates such as FRP, and selected engineered plastics. The toughened formulation offers excellent impact and peel strength together with extended working time to accommodate a wider range of assembly processes.

Key Features

  • Replaces welding, brazing, riveting and other mechanical fastening methods.
  • Bonds prepared and unprepared metals, FRP and selected engineered plastics with minimal substrate preparation.
  • Extended working time of 20–25 minutes to support larger or more complex assemblies.
  • High impact and peel strength with 100% elongation for improved fatigue resistance.
  • Service temperature from -40°F to +300°F (-40°C to +149°C).
  • Resists dilute acids, alkalis, solvents, greases, oils, moisture, salt spray, weathering and indirect UV exposure.

Suitable For

  • Structural metal bonding
  • FRP and composite bonding
  • Engineered plastic bonding
  • Automotive assembly
  • Industrial structural assembly

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber Paste
Density
Volumetric mass per unit
959-995 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
150000-550000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
59 °C

Additional Information

As-Supplied / Before-Processing Properties

Property Value
Appearance Amber paste
Viscosity 150,000–550,000 cP @ 77°F (25°C), Brookfield
Density 8.00–8.30 lb/gal (959–995 kg/m³)
Flash Point 59°F (15°C), Seta Closed Cup
Mix Ratio 10:1 by volume (Adhesive : LORD® Accelerator 25GB)
Mixed Appearance Red paste
Working Time 20–25 minutes @ 75°F (24°C)
Time to Handling Strength 50–70 minutes @ 75°F (24°C), 50 psi shear
Full Cure Time 5 hours @ 75°F (24°C)
Solids Content 100%

After-Processing / Final-State Properties

Property Value Test Method
Hardness Shore D 67 —
Tensile Strength at Break 2,683 psi (18.5 MPa) ASTM D638, modified
Elongation 100% ASTM D638, modified
Young's Modulus 125,000 psi (862 MPa) ASTM D638, modified
Glass Transition Temperature (Tg) 178°F (81°C) ASTM E1640-99 (DMA)