LORD 7701

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LORD 7701

Main features

  • Cured-Rubber/Urethane/Elastomer Adhesion Treatment
  • No-Mix Wipe/Brush/Dip/Flood Application
  • Compatible LORD Epoxy/Urethane Adhesives

Product Description

LORD® 7701 Adhesion Enhancer/Surface Modifier is a solvent-based surface treatment for cured and thermoplastic polymeric materials. It chemically alters elastomer surfaces to make them more receptive to bonding with compatible epoxy and urethane adhesives. LORD 7701 is designed for natural rubber, synthetic polyisoprene, SBR, butyl, polybutadiene, neoprene, EPDM, nitrile, polyurethane, styrenic block copolymers, and PVC. It requires no mixing, applies by wipe, brush, dip, or flood, and is ready for assembly after the ethyl-acetate solvent flashes off in less than five minutes. Do not apply LORD 7701 to metal surfaces.

Key features

  • Reactive surface treatment for cured rubber and thermoplastic elastomers
  • Functions as both a cleaner and surface conditioner
  • Requires no mixing or post-treatment rinse
  • Preferred wipe application with brush, dip, and flood alternatives
  • Less than five-minute solvent flash-off under suitable conditions
  • Improves adhesion to cured rubber and cast urethane
  • Supports compatible LORD epoxy and urethane adhesive systems

Applications

  • Cured-rubber-to-metal assemblies used with a compatible structural adhesive
  • Natural rubber, SBR, nitrile, EPDM, neoprene, and polyurethane treatment
  • Cast-urethane bonding processes
  • Thermoplastic elastomer and PVC surface conditioning

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear to Cloudy Liquid Density
Density
Volumetric mass per unit
870.0 - 930.0 kg/m3
Solids
2.3 - 3.5 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-4 °C

Additional Information

Reactive elastomer surface treatment

LORD® 7701 Adhesion Enhancer/Surface Modifier

A clear-to-cloudy, ethyl-acetate-based surface treatment that chemically modifies cured and thermoplastic elastomers before adhesive application. It is used with compatible LORD epoxy and urethane adhesives and must be applied to the rubber or polymer surface—not to the metal substrate.

No mixing Ethyl acetate <5 min flash-off Rubber and TPE treatment Do not apply to metal
LORD 7701 adhesion enhancer and surface modifier packaging

LORD 7701 adhesion enhancer and surface modifier packaging

As supplied

Low-solids reactive treatment in ethyl acetate

Property Typical value Context
Appearance Clear to cloudy liquid Visual condition; confirm acceptability against the controlled product specification.
Density 870–930 kg/m³ Equivalent to 7.3–7.8 lb/gal.
Solids content 2.3–3.5% by weight Low-solids reactive surface treatment.
Solvent Ethyl acetate Current SDS identifies approximately 95–100% ethyl acetate.
Flash point -4°C Seta method; highly flammable liquid and vapour.
Mixing None required Prevent contamination during transfer and application.
Compatible substrates and adhesive systems

Treat the elastomer surface before applying a compatible adhesive

Cured elastomers

Natural rubber, synthetic polyisoprene, SBR, butyl, polybutadiene, neoprene, EPDM, nitrile, and polyurethane.

Thermoplastic polymers

Styrene-butadiene and styrene-isoprene block copolymers, thermoplastic elastomers, and PVC after validation.

Compatible adhesive families

Published for use with a broad range of LORD epoxy and urethane adhesives used to bond cured rubber.

Metal restriction

Do not apply LORD 7701 to metal surfaces. Prepare the metal separately according to the selected adhesive system.

Surface preparation and application

Remove contamination and apply the minimum necessary treatment

  • Remove contamination from the rubber or polymer surface with a validated solvent wipe.
  • Transfer only the minimum required quantity into a new, clean, compatible container.
  • Use wiping as the preferred application method with a clean cotton rag.
  • Change wiping rags frequently as they collect contamination.
  • Brush with compatible bristle or foam brushes; use synthetic bristles.
  • Do not allow metal brush handles or collars to contact LORD 7701.
  • For dipping, rack treated parts so excess material can drain and the solvent can flash off.
  • Flood application is supported where contamination and excess-material control can be maintained.
  • Spray application is not recommended because of the material's reactivity.
  • Discard transferred or excess material; never return it to the original container.
LORD 7701 process showing rubber cleaning clean-container transfer wipe brush dip or flood application flash-off and adhesive bonding

LORD 7701 process showing rubber cleaning clean-container transfer wipe brush dip or flood application flash-off and adhesive bonding

Flash-off, assembly, and retreatment

Assemble shortly after the ethyl acetate flashes off

Flash-off

Treatment is complete after the solvent flashes off, typically in less than five minutes under suitable airflow.

No rinse

Rinsing is not required after the solvent has evaporated.

Assembly timing

Best bonds are obtained by assembling shortly after flash-off. Validate any treated-part storage interval.

Retreatment

Parts may be retreated when necessary, provided contamination and process compatibility are controlled.

Storage, handling, and safety

Shelf life is six months from date of shipment at 21–27°C in the original unopened container. Store in a cool, dark, well-ventilated area using the original or a compatible UV-filtering plastic or glass container. Do not store in metal containers. Keep away from oil, grease, sawdust, floor sweepings, readily oxidised organic materials, ammonia, amines, ammonia salts, metallic materials, water, and alcohol. The current US SDS classifies LORD 7701 as a highly flammable liquid and vapour that causes serious eye irritation, may cause drowsiness or dizziness, and is toxic to aquatic life with long-lasting effects. Use explosion-proof ventilation and electrical equipment, non-sparking tools, grounding and bonding, suitable gloves, protective clothing, and eye and face protection.

Bond performance evidence

Adhesion results depend on the complete treatment, adhesive, rubber, metal preparation, and cure system

Published 45° peel data used 0.3 × 15 × 2 cm rubber specimens bonded to grit-blasted steel and cured for 48 hours at room temperature. Epoxy testing used LORD 305-1/305-2 or LORD 320/310B systems. Values are typical and not specification limits.

Test system Rubber substrate Typical result Failure mode
Epoxy adhesive with LORD 7701 Natural rubber 40–50 pli 100% rubber failure
Epoxy adhesive with LORD 7701 SBR 105–120 pli 100% rubber failure
Epoxy adhesive with LORD 7701 Nitrile 75–85 pli 100% rubber failure
Cast polyurethane with LORD 7701 Natural rubber 105–120 pli in DS3223E; an older DS3461 copy reports a conflicting range 100% rubber failure
Cast polyurethane with LORD 7701 SBR 75–85 pli 100% rubber failure; stock break also reported
Cast polyurethane with LORD 7701 Nitrile 70–80 pli 100% rubber failure
Cast polyurethane with LORD 7701 Polychloroprene 40–50 pli 100% rubber failure

ASTM D429-B, 45° angle. Do not compare these values without preserving adhesive chemistry, rubber compound, metal preparation, specimen dimensions, cure, and failure mode.

Applications and process design

Control cleanliness, treatment coverage, flash-off, and time to adhesive application

LORD 7701 is appropriate where cured-rubber or elastomer adhesion is limited by surface chemistry and a compatible adhesive system is available. Final qualification should address rubber formulation and cure state, blooming, mould release, solvent-wipe compatibility, application method, coverage, contamination, airflow, flash-off, treated-part storage, retreatment, adhesive wetting, metal preparation, cure, environmental ageing, and desired failure mode.

Rubber-to-metal bonding

Apply LORD 7701 only to the rubber; prepare the metal according to the selected adhesive TDS.

Cast-urethane bonding

Use the treatment to improve wetting and adhesion to supported elastomer surfaces.

Controlled production cells

Use clean transfer containers, frequent rag replacement, compatible tools, and strict segregation from metal and reactive contaminants.

Product resources

LORD 7701 technical, safety, and bonding guidance

Technical Data Sheet — DS3461

LORD-branded technical data supporting substrate scope, application methods, flash-off, storage, typical properties, and bond-performance evidence.

Open resource
Current Surface Treatment Data — DS3223E

Current Parker technical data for the corresponding 7701 surface treatment, including application, storage, and performance details.

Open resource
Safety Data Sheet — LORD 7701

Current US safety information for flammability, exposure controls, handling, storage, spill response, transport, and disposal.

Open resource
Structural Adhesive Bonding Application Guide — AG1018

General substrate preparation, joint-design, adhesive application, fixturing, failure-mode, cleanup, and qualification guidance.

Open resource

Validate LORD® 7701 for your elastomer and adhesive combination

Krayden can help review rubber chemistry, surface contamination, application method, flash-off, tool and container compatibility, treated-part storage, adhesive selection, metal preparation, failure mode, environmental exposure, and production safety controls.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services