LORD 7650

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LORD 7650

Main features

  • One-Part Moisture-Cure Urethane
  • 15 to 30-Minute Solvent Flash
  • Multi-Material Foam/Fabric/Rubber/Plastic/Metal Bonding

Product Description

LORD® 7650 Urethane Adhesive is a single-component, solvent-borne, moisture-cure urethane adhesive that initially behaves like a contact adhesive and then permanently cross-links as cure develops. It bonds open-cell polyethylene foam, Styrofoam, urethane foam, plastic, fabric, rubber, and prepared metal. The honey-coloured liquid requires no mixing and can be applied by roll coat, spray, brush, or flow coat to one substrate surface. Typical published properties include 400–2,000 cP viscosity, 61–66% solids by weight, a 15–30 minute solvent-flash handling window, and complete cure in approximately 1–5 days, depending on the substrates and relative humidity.

Key features

  • Single-component moisture-cure urethane adhesive requiring no mixing
  • High initial tack and green strength after solvent flash
  • One-sided application unlike conventional two-sided contact adhesive
  • 400–2,000 cP viscosity for roll, spray, brush, or flow coating
  • Bonds foam, fabric, rubber, plastics, Styrofoam, and prepared metals
  • Good impact resistance and resistance to water and chemicals
  • Room-temperature cure without an oven or external heat source

Applications

  • Gaskets and foam laminations
  • Tank linings and rubber-to-substrate bonding
  • Automotive interiors and carpeting
  • Construction panels and flooring

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Tan Liquid
Density
Volumetric mass per unit
935 -1007 kg/m3
Solids
61-66 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
400 - 2000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-2 °C

Additional Information

Single-component solvent-borne moisture-cure urethane

LORD® 7650 Urethane Adhesive

A honey-coloured liquid adhesive that develops initial contact-like tack and then permanently cross-links through atmospheric moisture. It supports one-sided application and room-temperature processing for foam, fabric, rubber, plastics, Styrofoam, and prepared-metal assemblies.

One component Moisture cure 400–2,000 cP 15–30 min flash 1–5 day cure
LORD 7650 single-component urethane adhesive packaging

LORD 7650 single-component urethane adhesive packaging

As supplied

Low-viscosity honey-coloured liquid containing MEK and toluene

Property Typical value Test or claim context
Appearance Honey liquid Visual description in DS3459.
Viscosity 400–2,000 cP Brookfield LVT, spindle 2, 12 rpm.
Density 935–1,007 kg/m³ Equivalent to 7.8–8.4 lb/gal.
Solids content 61–66% by weight The balance includes volatile solvent.
Flash point 3°C Seta flash-point method; highly flammable processing implications.
Published solvents Methyl ethyl ketone and toluene Current SDS and local controls govern exposure and handling.
Surface preparation and application

Clean the substrate and apply to one bonding surface

  • Remove grease, dirt, dust, moisture, release agents, rust, and other contaminants.
  • For plastics, use a dry-rag wipe or a validated solvent-dampened rag.
  • For metals, prime or grit blast and then solvent wash for optimum performance.
  • For cured rubber, apply LORD 7701 and allow it to flash off before LORD 7650 application.
  • Apply by roll coat, spray, brush, or flow coat.
  • Apply to one substrate side only; a conventional two-sided contact-adhesive process is not required.
  • Control wet-film coverage, overspray, edge migration, and solvent ventilation.
  • Mate parts only after the required flash condition is achieved and the application remains within the validated assembly window.
LORD 7650 process showing substrate cleaning one-sided roll spray brush or flow application solvent flash mating and moisture cure

LORD 7650 process showing substrate cleaning one-sided roll spray brush or flow application solvent flash mating and moisture cure

Solvent flash and moisture cure

Separate the handling-strength flash stage from final cross-linking

Initial flash

Handling strength is achieved after approximately 15–30 minutes of solvent flash.

Final cure

Complete moisture cure takes approximately 1–5 days, depending on the substrates and relative humidity.

Humidity dependence

Low moisture availability, impermeable substrates, thick films, or sealed joints can slow cure development.

No heat required

The system cures without an oven or external heat source, but the actual environment must still be qualified.

Storage and industrial safety

Shelf life is six months from date of shipment when stored at 21–27°C in the original unopened container. After opening, protect the adhesive from moisture with approved desiccant cartridges or dry nitrogen. LORD 7650 has a published 3°C flash point and contains MEK and toluene. Use only with trained personnel, explosion-appropriate process controls, effective ventilation, ignition-source control, suitable personal protection, and the current regional SDS and package label. The supplied file identified only as “rehsfil0” could not be verified as a readable product-specific safety document.

Bond performance

Substrate-specific peel results after 48 hours at 50% relative humidity

The TDS reports bond strength in pounds per linear inch after a 48-hour cure at 50% RH. Failure modes are important: foam tear, thin-rubber tear, or rubber tear indicate substrate failure under the stated test rather than a universal adhesive-strength limit.

Substrate combination Typical bond strength Reported failure mode
Polyethylene foam to aluminium or steel 15–18 pli Foam tear
Vinyl to foam 5–8 pli Foam tear
Vinyl to aluminium 30–35 pli Not stated in the table
Rubber to metal 15–20 pli Thin rubber tear
Styrofoam to epoxy-primed galvanised steel 15–20 pli Foam tear
Rubber to concrete 14–17 pli Rubber tear
Applications and joint design

Use initial tack for assembly while allowing moisture access for final cure

Published applications include gaskets, tank linings, automotive interiors, carpeting, construction panels, and flooring. Final qualification should address substrate porosity, solvent sensitivity, foam attack, wet-film coverage, flash time, open time, humidity access, cure depth, trapped solvent, odour, emissions, vertical flow, press or fixture requirements, cleaning, water and chemical exposure, and long-term environmental durability.

Foam and fabric laminations

Open-cell polyethylene foam, urethane foam, Styrofoam, fabric, vinyl, and carpet constructions after compatibility testing.

Rubber assemblies

Gaskets, linings, and rubber-to-metal or rubber-to-concrete joints using the specified surface treatment where required.

Interior and construction panels

Automotive interiors, construction panels, and flooring where solvent flash and cure ventilation can be controlled.

Product resources

LORD 7650 technical and bonding guidance

Technical Data Sheet — DS3459

Product-specific technical data for substrates, preparation, application, solvent flash, moisture cure, storage, as-supplied properties, and bond results.

Open resource
Structural Adhesive Bonding Application Guide — AG1018

General joint-design, surface-preparation, application, fixturing, failure-mode, cleanup, and qualification guidance.

Open resource
LORD Structural Adhesives Selector Guide — SG1018

General LORD adhesive selection context. Product-specific values remain governed by DS3459.

Open resource

Validate LORD® 7650 for your foam, rubber, fabric, or panel assembly

Krayden can help review substrate preparation, coating method, wet-film coverage, one-sided application, solvent flash, ventilation, humidity access, cure time, foam compatibility, bond testing, and production safety controls.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services