LORD 7550A Urethane Adhesive

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

LORD 7550A Urethane Adhesive

Main features

  • Equal-Mix LORD 7550 Resin Component
  • 1,800 to 4,000 cP Viscosity
  • Lexan, ABS, and Primed-Metal Bonding

Product Description

LORD® 7550A Urethane Adhesive Resin is the resin component of the equal-mix LORD 7550 two-component clear urethane adhesive system. When combined 1:1 by volume with LORD 7550C curative, the system bonds Lexan, ABS, polycarbonate, other plastics, and properly prepared and primed metals. The clear-to-yellow liquid resin has a typical viscosity of 1,800 to 4,000 cP at 25°C. The mixed adhesive is self-leveling, has a typical working time of three to five minutes, reaches handling strength in approximately 60 minutes, and cures to full strength in about 72 hours at room temperature.

Key features

  • LORD 7550 resin component: LORD 7550A is mixed 1:1 by volume with LORD 7550C curative.
  • Low-viscosity liquid resin: Typical component viscosity is 1,800 to 4,000 cP at 25°C.
  • Clear urethane bonding system: The paired system is documented for plastics and properly prepared and primed metals.

Applications / Suitable for

  • Resin component of the LORD 7550 urethane adhesive system
  • Bonding Lexan, ABS, polycarbonate, and other plastics
  • Bonding properly prepared and primed metals

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear to Clear Yellow Liquid
Density
Volumetric mass per unit
1150 -1174 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1800 - 4000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>93 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Component role Resin N/A LORD 7550A
Appearance Clear to clear-yellow liquid N/A As supplied
Viscosity 1,800 to 4,000 cP At 25°C
Density 1,150 to 1,174 kg/m³ As supplied
Flash point >93 °C Closed cup
Shelf life 6 months At 21°C to 27°C in the original unopened container