LORD 7550

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LORD 7550

Main features

  • Optically Clear Bonding
  • 3 to 5-Minute Working Window
  • Weathering/Humidity/Salt-Spray/UV Environmental Resistance

Product Description

LORD® 7550-A/C Urethane Adhesive is an equal-mix, two-component, optically clear urethane adhesive system for bonding Lexan®, ABS, polycarbonate, other plastics, and properly prepared or primed metals. The self-levelling material flows into narrow or difficult-to-reach spaces and is suited to tight-tolerance and appearance-sensitive assemblies. LORD 7550-A resin and LORD 7550-C curative mix 1:1 by volume to provide a typical 3–5 minute working time at 24°C, 2–3 minute purge time, approximately 60 minutes to handling strength at 25°C, and full cure in approximately 72 hours at room temperature.

Key features

  • Optically clear, equal-mix two-component urethane adhesive
  • Self-levelling flow for narrow gaps and difficult-to-reach spaces
  • Simple 1:1 volumetric mix ratio
  • 3–5 minute working time with approximately one-hour handling strength
  • Weathering, humidity, salt-spray, and UV-resistance positioning
  • Solvent resistance after cure
  • Typical 0.2 W/m·K thermal conductivity reported in the LED selector guide

Applications

  • Optics, lenses, diffusers, and transparent plastic bonding
  • LED cases, luminaires, cable connectors, and related assemblies
  • Trimcap, letter-track, channel-letter, and aesthetic sign assemblies
  • Lexan®, ABS, polycarbonate, and validated primed-metal joints

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
A (Resin)/B(Curative): Clear to Clear Yellow Liquid
Density
Volumetric mass per unit
A (Resin): 1150 -1174 | B(Curative): 1078 -1126 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
A (Resin): 1800 - 4000 | B (Curative): 6000 -12,500 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
A (Resin)/ B(Curative): >93 °C

Additional Information

Optically clear equal-mix urethane adhesive

LORD® 7550-A/C Urethane Adhesive

A clear, self-levelling, two-component urethane system for transparent plastics, tight-tolerance interfaces, LED assemblies, sign components, and validated primed-metal joints. Its low-viscosity flow helps the mixed adhesive enter narrow or difficult-to-reach spaces.

Optically clear Self-levelling 1:1 by volume 3–5 min work time 72 h full cure
LORD 7550-A resin and LORD 7550-C curative packaging

LORD 7550-A resin and LORD 7550-C curative packaging

As supplied and mixed

Clear components for equal-volume cartridge dispensing

Property LORD 7550-A resin LORD 7550-C curative Mixed system
Appearance Clear to clear-yellow liquid Clear to clear-yellow liquid Optically clear
Viscosity at 25°C 1,800–4,000 cP 6,000–12,500 cP No product-specific mixed-viscosity value published in DS3451
Density 1150–1174 kg/m³ 1078–1126 kg/m³ Use component data for material calculations
Flash point >93°C, closed cup >93°C, closed cup Follow both current SDS documents
Mix ratio 1:1 resin-to-curative by volume
Solids content 100% by weight
Working time at 24°C 3–5 minutes using a 12.7 mm bead condition
Purge time at 24°C 2–3 minutes
Handling-strength time at 25°C Approximately 60 minutes
Surface preparation, mixing, and application

Clean the surfaces, dispense 1:1, purge, and assemble within the short work window

  • Remove grease, dirt, dust, release agents, and other contamination.
  • For plastics, wipe with a dry rag or a validated solvent-dampened rag.
  • For metals, grit blast and solvent wash, then prime for optimum bond performance.
  • Use an equal-volume cartridge or validated 1:1 meter/mix system.
  • Level the component flow before attaching the mixer.
  • Purge the mixed adhesive during the published 2–3 minute purge interval.
  • Apply with a handheld cartridge and assemble parts within 3–5 minutes.
  • Control flow and edge containment because the material is self-levelling.
  • Prevent bubbles, surface contamination, and optical defects in appearance-sensitive joints.
Mixpac™ Dispensing Systems for Parker Lord Two Component Material

Mixpac™ Dispensing Systems for Parker Lord Two Component Material

Cure, cleanup, and rework

Allow approximately 72 hours for full room-temperature cure

Handling strength

Approximately 60 minutes at 25°C under the published bead condition.

Full cure

Approximately 72 hours at room temperature.

Uncured cleanup

Clean equipment before cure with acetone or MEK. Do not use alcohol.

Cured removal

Heating to approximately 149°C or above may soften the cured adhesive for separation. Validate substrate and optical-part heat tolerance.

Storage and industrial safety

Shelf life is six months when stored at 21–27°C in a clean, dry environment in the original unopened containers. After opening, protect both components from excessive moisture using approved desiccant cartridges or dry nitrogen. The supplied EHS identifiers were not available as readable product-specific SDS documents. Confirm and review the current regional SDS for both LORD 7550-A resin and LORD 7550-C curative before handling, mixing, cleanup, transport, storage, or disposal.

Performance characteristics

Optical clarity, environmental resistance, and low bulk thermal conductivity

DS3451 does not publish tensile, elongation, modulus, lap-shear, peel, hardness, or dielectric values. Do not add structural-property claims without separate product-specific evidence.

Characteristic Published positioning or value Claim control
Optical appearance Optically clear Validate clarity, yellowing, haze, bubbles, and interface appearance in the finished assembly.
Flow behaviour Self-levelling Provide edge containment where uncontrolled flow would be unacceptable.
Thermal conductivity 0.2 W/m·K Selector-guide value from SG1013; typical and not a thermal-management claim.
Weathering and humidity Environmentally resistant Supplier positioning; no numerical exposure duration in DS3451.
Salt spray Resistant No product-specific numerical test duration published in DS3451.
UV exposure UV resistant Validate long-term colour and optical transmission for the actual exposure.
Solvent resistance Solvent resistant after cure Validate the actual paint, cleaner, solvent, duration, and temperature.
Applications and design considerations

Use clear, self-levelling flow for tight-tolerance and appearance-sensitive assemblies

Published applications include optics bonding, cases and diffusers, cable connectors, case and luminaire sealing, trimcap, letter track, aesthetic assemblies, and selected potting or encapsulation tasks. Final qualification should address substrate grade, stress cracking, primer, joint gap, edge containment, bubble control, cure shrinkage, optical clarity, haze, yellowing, UV exposure, water ingress, cleaner compatibility, thermal expansion, and service temperature.

LED and optical assemblies

Optics, lenses, diffusers, housings, cable connectors, and luminaires requiring clear adhesive flow.

Sign fabrication

Trimcap, letter track, channel-letter, and aesthetic assemblies using compatible plastics.

Tight-tolerance interfaces

Self-levelling flow into narrow spaces where edge control and bubble prevention can be maintained.

Product resources

LORD 7550-A/C technical and application guidance

Technical Data Sheet — DS3451

Controlling product-specific TDS for component properties, mixing, work time, purge time, handling strength, cure, storage, and use guidance.

Open resource
Electronic Materials for LED Applications — SG1013

LED application context and selector-guide values, including 0.2 W/m·K thermal conductivity and 72-hour room-temperature cure.

Open resource
Structural Adhesive Bonding Application Guide — AG1018

General guidance for substrate preparation, joint design, cartridge purging, mixing, fixturing, cleanup, and rework.

Open resource
LORD Structural Adhesives Selector Guide — SG1018

General product-selection and adhesive-system context.

Open resource
LORD Urethane Adhesives for the Sign Industry — PB8268

Product-specific sign-industry positioning for trimcap, letter track, aesthetic assemblies, and optically clear bonding.

Open resource

Validate LORD® 7550-A/C for your clear plastic or LED assembly

Krayden can help review substrate compatibility, primer, cartridge and mixer selection, purge, self-levelling flow, edge containment, work time, optical appearance, UV exposure, environmental sealing, cure, cleaning, and final assembly qualification.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services