LORD 7542D

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 7542D

Main features

  • Equal 1:1 Volume Mixing
  • 20-30 Minute Working Time
  • 70% Cured Elongation

Product Description

LORD 7542D Urethane Adhesive is the 7542-A resin and 7542-D curative configuration of an equal-mix, two-component urethane adhesive for bonding FRP, SMC, other plastics, and primed metals. The system mixes 1:1 by volume and provides a typical 20 to 30 minute working time at 24 deg C, followed by handling strength in approximately 3 hours. A recommended 254 to 1016 um bondline supports controlled assembly, and full strength develops in 24 hours or less at 24 deg C. The cured adhesive has a typical tensile strength of 18.70 MPa and 70% elongation.

Key features

  • Equal 1:1 Volume Mix: Uses the same volume of 7542-A resin and 7542-D curative.
  • 20-30 Minute Working Time: Provides a defined assembly window at 24 deg C.
  • 70% Cured Elongation: Combines urethane bonding with a flexible cured response.

Applications / Suitable for

  • Bonding FRP, SMC, and other plastics with limited surface preparation.
  • Bonding primed metal substrates.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Tan Liquid
Density
Volumetric mass per unit
1234 -1270 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
5000 -14,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>93 °C

Additional Information

Technical properties

7542-A resin and 7542-D curative properties

Values apply to the 7542-A resin and 7542-D curative configuration.

Property Value Unit Method / condition
7542-A resin appearance Dark brown liquid As supplied; typical
7542-D curative appearance Tan liquid As supplied; typical
7542-A resin viscosity 1,500 to 4,500 mPa s 25 deg C; typical
7542-D curative viscosity 5,000 to 14,000 mPa s 25 deg C; typical
7542-A resin density 11.45 to 11.75 lb/gal As supplied; typical
7542-D curative density 10.3 to 10.6 lb/gal As supplied; typical
Flash point >93 deg C Closed cup; both components; typical
Mix ratio 1:1 by volume 7542-A resin : 7542-D curative
Technical properties

Mixed and cured adhesive properties

Cured-property values apply to the LORD 7542 adhesive system.

Property Value Unit Method / condition
Working time 20 to 30 min 24 deg C, 12.7 mm bead; typical
Handling-strength time 3 h 24 deg C, 12.7 mm bead; typical
Time to full strength 24 or less h 24 deg C
Recommended bondline thickness 254 to 1016 um For optimum adhesion
Hardness 87 Shore A ASTM D2240; typical cured material
Tensile strength at break 18.70 MPa ASTM D638; typical cured material
Elongation at break 70 % ASTM D638; typical cured material
Glass transition temperature 46 deg C ASTM D3418; typical cured material

Leading Brands Trust in Our Products and Services