Main features

  • 1:1 Medium-Work-Time Urethane Curative
  • 10 to 20-Minute Working Time
  • 60 to 120-Minute Handling Time

Product Description

LORD® 7542-C Urethane Adhesive Curative is Part 2 of the LORD 7542-A/C two-component structural urethane adhesive system. It must be combined 1:1 by volume with LORD 7542-A resin before use. LORD 7542-C is supplied as a tan liquid with a typical 4,000–14,000 cP viscosity at 25°C. When mixed with LORD 7542-A, the system provides a typical 11–15 minute working time at 24°C, approximately 2 hours to handling strength, and full strength in 24 hours or less.

Key features

  • Curative component for the LORD 7542-A/C structural urethane adhesive system
  • Equal-volume 1:1 mixing with LORD 7542-A resin
  • Intermediate 11–15 minute working time for balanced assembly speed
  • Suitable for cartridge or automatic meter/mix/dispense processing
  • Supports FRP, SMC, CFRP, plastics, and prepared or coated metal bonding
  • System-level typical tensile strength of 18.7 MPa with 70% elongation
  • Documented system-level resistance to humidity, salt spray, water, and temperature exposure

Applications

  • Composite panel and enclosure assembly requiring a medium working window
  • Heavy-duty truck, service-truck, trailer, and vehicle-accessory bonding
  • SMC, FRP, and CFRP structural joints
  • Prepared or powder-coated metal-to-composite assemblies

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Tan Liquid
Density
Volumetric mass per unit
1234 -1270 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
4000 -14,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>93 °C

Additional Information

Curative component for a medium-work-time 1:1 urethane system

LORD® 7542-C Urethane Adhesive Curative

LORD 7542-C is Part 2 of 2 in the LORD 7542-A/C structural urethane adhesive system. It is not used alone. Combine it 1:1 by volume with LORD 7542-A resin to obtain an intermediate assembly window between the faster 7542-B and longer-work-time 7542-D systems.

Curative component Tan liquid 4,000–14,000 cP 1:1 by volume 11–15 min work time
LORD 7542-C urethane adhesive curative packaging

LORD 7542-C urethane adhesive curative packaging

As supplied

Tan liquid curative for controlled equal-volume mixing

Property Typical value Context
Component role Curative, Part 2 of 2 Must be combined with LORD 7542-A resin before use.
Appearance Tan liquid LORD 7542-C component.
Viscosity at 25°C 4,000–14,000 cP Component viscosity; not mixed-system viscosity.
Density Published in DS3444 Use the current controlled value for weight-ratio or consumption calculations.
Flash point >93°C, closed cup Does not eliminate decomposition, heated-process, or fire hazards.
Mix ratio 1:1 by volume with LORD 7542-A resin Use equal-volume cartridges or validated meter/mix equipment.
Required resin and process window

Use only with LORD 7542-A resin at the documented 1:1 volumetric ratio

Required companion

LORD 7542-A resin. LORD 7542-C is not a complete stand-alone adhesive.

Working time

11–15 minutes at 24°C using the supplier's 12.7 mm bead condition.

Handling strength

Approximately 2 hours at 24°C under the published test basis.

Full strength

The mixed system reaches full strength in 24 hours or less at 24°C.

Surface preparation, mixing, and application

Prepare the substrates and combine 7542-C with 7542-A before the medium work window expires

  • Remove grease, dirt, moisture, release agents, and other contaminants.
  • For plastics, use a dry-rag wipe or a validated solvent-dampened rag.
  • For metals, the TDS recommends priming or powder coating.
  • Use equal-volume cartridges or automatic meter/mix/dispense equipment.
  • Level cartridge plungers before attaching the mixer.
  • Purge at least one mixer length before applying adhesive to the substrate.
  • Mate parts within the 11–15 minute working time.
  • Clamp until the mixed system reaches handling strength.
  • Maintain a typical 254–1016 µm bondline for optimum adhesion.
Mixpac Dispensing System for Two Component Parker Lord Materials

Mixpac Dispensing System for Two Component Parker Lord Materials

Cure, cleanup, and rework

Cure and final properties apply only after correct mixing with LORD 7542-A

Cure

Full system strength develops in 24 hours or less at 24°C.

Uncured cleanup

Clean equipment and tools before cure with acetone or MEK. Do not use alcohol.

Cured removal

Heating the cured adhesive to approximately 149°C or above may soften it for separation; validate substrate heat resistance.

Painting and cleaning

Painting and most cleaning processes are not expected to reduce bond strength under the supplier's system-level guidance.

Storage and industrial safety

LORD 7542-C is one of the curatives specifically excluded from the TDS warning about prolonged exposure below 10°C, but it should still be stored within the published 18–30°C shelf-life range in its original unopened container. A product-specific LORD 7542-C SDS was not supplied. Do not infer its hazard classification from the LORD 7542-B SDS. Obtain and review the current regional 7542-C SDS and package label before handling, and use the required ventilation, personal protection, storage, spill, transport, and disposal controls.

System-level cured properties and bond performance

Do not assign final structural properties to LORD 7542-C curative by itself

LORD 7542-C is an uncured component. Final-state values apply only to a correctly metered, mixed, and cured LORD 7542-A/C adhesive system. DS3444 presents the bulk cured-property table at family level and does not explicitly identify the curative used.

Property Typical system-level value Context
Hardness 87 Shore A ASTM D2240, Method A.
Tensile strength at break 18.70 MPa ASTM D638.
Elongation 70% ASTM D638.
Young’s modulus 83.6 MPa ASTM D638.
Glass-transition temperature 46°C ASTM D3418.
Moisture absorption 1.65% ASTM D570.

Selected family-level room-temperature lap-shear results include 4.10 MPa on SMC, 17.90 MPa on e-coated steel, and 22.10 MPa on CFRP under the documented preparation, bondline, area, 1:1 mix, and 24-hour room-temperature cure. Confirm that these results apply to the A/C formulation before treating them as variant-specific.

Applications and joint design

Choose 7542-C where a balanced assembly window is more useful than the fastest or longest option

The LORD 7542-A/C system is positioned for SMC, FRP, CFRP, plastics, e-coated steel, powder-coated metals, truck and trailer structures, vehicle accessories, and other composite assemblies. Final qualification must address the 11–15 minute work window, equipment and mixer residence time, substrate and coating, bondline, joint geometry, clamping, peel, impact, fatigue, temperature, water and humidity exposure, painting, rework, and required failure mode.

Product resources

LORD 7542-C selection, processing, and application guidance

Technical Data Sheet — DS3444

Controlling technical data for LORD 7542-C curative, the required LORD 7542-A resin, process window, storage, system-level cured properties, and bond performance.

Open resource
Two-Component Urethane Adhesives Brochure — PB8224

Family comparison covering LORD 7542 systems and curative-selection context.

Open resource
Structural Adhesive Bonding Application Guide — AG1018

Joint design, substrate preparation, cartridge purging, bondline, fixturing, failure-mode, and rework guidance.

Open resource
LORD Structural Adhesives Selector Guide — SG1018

General structural-adhesive selection and market context.

Open resource
Service Work Trucks Selector Guide — SG1031

Application context for service-body panels, compartments, roofs, and mixed-material structures.

Open resource
Utility and Class Eight Trailers Selector Guide — SG1030

Application context for utility and Class Eight trailer structures.

Open resource

Validate LORD® 7542-C with LORD 7542-A for your assembly window

Krayden can help review 1:1 package and equipment configuration, mixer choice, 11–15 minute work time, substrate preparation, bondline, clamping, storage, safety documentation, environmental durability, and final assembly qualification.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers