LORD 7100A

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LORD 7100A

Main features

  • High-Strength Structural Bonding
  • Primerless Bonding to Many Plastics
  • VOC-Free Weathering/Aging-Resistant Urethane

Product Description

LORD® 7100-A/B Urethane Adhesive is a two-part, high-strength urethane adhesive formulated for bonding cloth, paper, plastics, foams, rubber, painted metals and powder-coated metals. The system combines an isocyanate-based 7100-A resin with a polyol-based 7100-B curative and can be cured at room temperature or with elevated heat for faster processing. Once cured, it forms a glossy black bond with resistance to solvents, weathering and aging.

Key Features

  • Broad substrate capability for cloth, paper, plastics, foams, rubber, painted metals and powder-coated metals.
  • High-strength plastic bonding without crazing, attacking or reducing the strength of the plastic substrate.
  • Primer reduction on many plastics to help lower material and labor requirements.
  • Solvent-, weathering- and aging-resistant performance after cure, with no VOC content or ozone-depleting chemicals.

Applications / Suitable for

  • Plastic and foam assemblies
  • Rubber bonding
  • Cloth and paper laminations
  • Painted-metal and powder-coated-metal assemblies

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
A (Resin)/ B(Curative): Black Liquid
Density
Volumetric mass per unit
A (Resin): 1486 -1522 | B(Curative): 1306 -1366 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
A (Resin): 3000 -16,000 | B (Curative): 45,000 - 72,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
A (Resin)/ B(Curative): >93 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed-system properties for LORD® 7100-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.

Property 7100-A Resin 7100-B Curative Mixed System Method / Condition
Composition Isocyanate-based resin Polyol-based curative Two-part urethane Product description
Appearance Black liquid Black liquid — Typical
Viscosity 3,000–16,000 cP 45,000–72,000 cP — At 77°F (25°C); resin: Brookfield LVT, Spindle 4, 30 rpm; curative: Brookfield HA, Spindle 6, 20 rpm
Density 12.4–12.7 lb/gal
(1486–1522 kg/m³)
10.9–11.4 lb/gal
(1306–1366 kg/m³)
— Typical
Flash Point >200°F
(>93°C)
>200°F
(>93°C)
— Closed cup
Mix Ratio 1 part 2 parts by volume
1.78 parts by weight
1:2 by volume
1:1.78 by weight
Resin to curative
Solids Content — — 100% Mixed adhesive
Working Time — — 5–10 minutes At 75°F (24°C)
Purge Time — — 3 minutes At 77°F (25°C)
Time to Handling Strength — — 2–3 hours At 73°F (23°C)
Shelf Life 6 months 6 months — Store at 65–85°F (18–30°C) in a clean, dry environment in the original, unopened container
Technical Properties

After-Processing / Final-State Properties

Supported cure and final-state characteristics for LORD® 7100-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Full Cure Time 24 hours At room temperature, 77°F (25°C); elevated temperatures accelerate cure
Cured Appearance Glossy black — Typical