LORD 4688

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 4688

Main features

  • Low-Density Honeycomb-Core Syntactic Reinforcement
  • Thixotropic Application Control
  • 30-Minute Working Window

Product Description

LORD® 4688 A/B Modified Epoxy Syntactic Foam is a two-component, low-density epoxy paste used to reinforce honeycomb core and other hollow structures. The smooth, creamy, thixotropic mixed material is suited to trowel or injection application. Pink Part A and blue Part B are combined at 100 parts A to 11 parts B to produce a brown mixture with a typical 30-minute working time at 24°C and approximately one-hour set time. The system cures in 24 hours at 24°C or 3 hours at 75°C. A typical specific gravity of 0.45 supports lightweight structural fill and reinforcement applications.

Key features

  • Low-density modified epoxy syntactic foam system
  • Smooth, creamy and thixotropic mixed consistency
  • Suitable for trowel or injection application
  • 100:11 Part A-to-Part B mix ratio
  • 30-minute working time at 24°C
  • Room-temperature or accelerated heat cure
  • ASTM E595 outgassing data reported in the source TDS

Applications

  • Honeycomb-core reinforcement
  • Hollow-structure filling and reinforcement
Product Family

LORD 4688

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
A: Pink Paste | B: Blue Paste | Mixed: Brown Paste
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:11
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.45
Physical Properties
Viscosity (Part B)
50 mPa.s

Additional Information

Low-density two-component epoxy syntactic foam

LORD® 4688 A/B Modified Epoxy Syntactic Foam

A lightweight modified epoxy syntactic foam system used to reinforce honeycomb core and other hollow structures. The mixed material has a smooth, creamy and thixotropic consistency suited to controlled trowel or injection placement.

Two component Specific gravity 0.45 Thixotropic mixed paste 30 min work time Room or heat cure
LORD 4688 Part A and Part B modified epoxy syntactic foam packaging

LORD 4688 Part A and Part B modified epoxy syntactic foam packaging

As supplied

Color-coded components for controlled mixing

Property Part A Part B Mixed system
Form Paste Liquid component Paste
Color Pink Blue Brown
Viscosity / rheology Thixotropic paste 50 cP Thixotropic
Mix ratio 100 parts Part A to 11 parts Part B; the source does not specify whether this basis is by weight or volume.
Flash point Greater than 125°C
Specific gravity 0.45 g/cm³ as reported; equivalent density statement in the source is 28.4 lb/ft³
Mixing, application and cure

Mix the color-coded components and place by trowel or injection

  • Condition both components to the intended processing environment before mixing.
  • Combine 100 parts Part A with 11 parts Part B using the validated ratio basis.
  • Mix until the pink and blue components form a uniform brown material.
  • Use trowel application for accessible cavities and injection where the assembly geometry supports controlled filling.
  • Complete placement within the typical 30-minute working time at 24°C.
  • Allow approximately one hour for set under the source conditions.
  • Cure for 24 hours at 24°C or 3 hours at 75°C.
  • Validate fill quality, voiding, exotherm, section thickness and cure temperature in the actual hollow structure.
Mixpac™ Dispensing Systems for Parker Lord Two Component Material

Mixpac™ Dispensing Systems for Parker Lord Two Component Material

Storage and handling

Shelf life is six months when stored in the original unopened containers in a clean, dry warehouse environment. The uploaded source does not provide a controlled storage-temperature range. Use only with adequate ventilation and suitable gloves and protective clothing. Obtain and follow current regional safety data for both components before production use.

Final properties and performance evidence

Low-density cured reinforcement with source-reported mechanical and outgassing data

The source identifies all values as indicative rather than design requirements. Mechanical units are not shown in the source and therefore are not assigned on this page.

Property Condition Source-reported value Interpretation boundary
Compression Room temperature 3,500 Units and method are not identified in the source.
Compression -320°F 8,000 Units and method are not identified in the source.
Tensile shear Room temperature 2,000 Substrate, specimen, units and method are not identified.
Tensile shear -320°F 1,500 Substrate, specimen, units and method are not identified.
Total mass loss ASTM E595 0.52% Typical outgassing result; assembly suitability still requires validation.
Collected volatile condensable material ASTM E595 0.01% Typical outgassing result; not a qualification by itself.

The material is positioned for reinforcing honeycomb core and other hollow structures. Final evaluation should address cavity geometry, injection path, fill completeness, trapped air, mass, cure exotherm, thermal expansion, low-temperature loading, substrate compatibility and the required structural margin.

Evaluate LORD® 4688 A/B for your honeycomb or hollow-structure reinforcement process

Krayden can help review ratio control, mixing, trowel or injection equipment, cavity access, fill verification, working time, cure schedule, outgassing requirements, low-temperature testing and final assembly qualification.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers