LORD 406/19GB

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LORD 406/19GB

Main features

  • 4:1 Metal-to-Plastic Bonding
  • 6 to 10-Minute Working Window
  • 18.6 MPa Cured Tensile Strength

Product Description

LORD® 406/19 Acrylic Adhesive is a two-component structural acrylic system consisting of LORD 406 adhesive and LORD Accelerator 19. Mixed at 4:1 by volume or approximately 3.02:1 by weight, the non-sag adhesive bonds many prepared or minimally prepared metals and engineered thermoplastics. It provides a typical 6–10 minute working time at 24°C, 12–17 minute handling-strength time, and 24-hour full cure. Typical cured properties include 18.6 MPa tensile strength, 30% elongation, 896 MPa Young’s modulus, and a 72°C glass-transition temperature.

Key features

  • Dedicated LORD 406 adhesive and Accelerator 19 structural acrylic system
  • Simple 4:1 volumetric mix ratio for cartridge or meter/mix processing
  • Non-sag paste for vertical and overhead application
  • High impact and peel performance, including low-temperature environments
  • Accelerator 19 supports improved high-temperature resistance
  • Room-temperature cure with handling strength in 12–17 minutes
  • UL 746C positioning for the 406/19 system, subject to the current listed construction

Applications

  • Bare, galvanised, stainless, and powder-coated metal assemblies
  • Engineered thermoplastics including polycarbonate, ABS, acrylic, and validated blends
  • Signs, enclosures, truck and trailer structures, and vehicle accessories
  • Bonded assemblies that undergo a validated e-coat or powder-coat bake

Technical Specifications

General Properties
Color
The color
Off-White to Tan Paste
Density
Volumetric mass per unit
1090 -1162 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
15 °C
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
72 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
100000 to 300000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
30 %

Additional Information

4:1 structural acrylic adhesive system

LORD® 406/19 Acrylic Adhesive

A dedicated two-component system combining LORD 406 adhesive with LORD Accelerator 19. The off-white-to-tan adhesive and off-white accelerator produce a tan mixed paste for structural bonding of metals and engineered plastics. Accelerator 19 is the selected cure component for improved high-temperature resistance and the system's published UL 746C positioning.

LORD 406 + Accelerator 19 4:1 by volume Non-sag 6–10 min work time 12–17 min handling
LORD 406 acrylic adhesive and LORD Accelerator 19

LORD 406 acrylic adhesive and LORD Accelerator 19 packaging

As supplied and mixed

LORD 406 adhesive and Accelerator 19 at a controlled 4:1 ratio

Property LORD 406 adhesive LORD Accelerator 19 406/19 mixed system
Appearance Off-white to tan paste Off-white paste Tan paste
Viscosity at 25°C 100,000–300,000 cP 20,000–70,000 cP No single mixed-viscosity value published
Density 1090–1162 kg/m³ 1467–1515 kg/m³ Use component data and actual ratio for material calculations
Flash point 15°C >93°C Follow both current SDS documents
Mix ratio 4:1 adhesive-to-accelerator by volume; approximately 3.02:1 by weight
Solids content 100%
Working time at 24°C 6–10 minutes
Handling-strength time at 24°C 12–17 minutes, based on the supplier's 60 psi shear criterion
Full cure at 24°C 24 hours
Surface preparation, mixing, and application

Prepare the substrate, purge the 4:1 cartridge, and apply before the working time expires

  • Remove grease, loose contamination, and poorly adhering oxides from metals.
  • Normal mill oils and drawing compounds may be tolerated, but actual production surfaces must be tested.
  • Clean engineered plastics and abrade only where required for optimum adhesion.
  • Level cartridge plungers before attaching the correct 4:1 mixer.
  • Discard the initial purge until a uniform tan colour confirms proper mixing.
  • Use handheld cartridges or automatic meter/mix/dispense equipment configured for 4:1 by volume.
  • Apply and mate parts within the 6–10 minute working window.
  • Use sufficient pressure for complete wet-out without starving the bondline.
LORD 406 19 on 4 to 1 cartridge mixing bead application

LORD 406 19 acrylic adhesive process showing surface preparation 4 to 1 cartridge levelling static mixing bead application part mating and fixturing

Cure, fixturing, and powder coating

Do not move or post-bake the assembly before handling strength

Work window

6–10 minutes at 24°C. Higher adhesive, substrate, or ambient temperature reduces available time.

Handling strength

12–17 minutes at 24°C under the TDS criterion. Fixture longer when joint load, mass, or geometry requires it.

Full cure

24 hours at 24°C before using full cured-property data as the design basis.

Post-bake processing

The LORD acrylic family has documented powder-coat-bake capability, but the strongest 204°C/90-minute statement in DS3882 is specifically tied to LORD 406/19GB. Validate 406/19 separately.

Storage and industrial safety

LORD 406 is the flammable component of the 406/19 system and has a published 15°C flash point. The supplied EHS identifier was not available as a readable product-specific document. Confirm the current regional SDS for LORD 406 and LORD Accelerator 19 before publication or use. Follow both labels for ventilation, ignition control, personal protection, spill response, storage, transport, and disposal.

Cured properties and bond performance

Published cured and joint data for LORD 406 with Accelerator 19

The values below are typical, not specification limits. Joint results remain tied to the stated substrate, surface condition, bondline, cure, specimen geometry, and test environment.

Property or joint Typical result Context
Tensile strength at break 18.6 MPa Modified ASTM D638; 406/19.
Elongation 30% Modified ASTM D638.
Young’s modulus 896.3 MPa Modified ASTM D638.
Glass-transition temperature 72°C ASTM E1640 by DMA.
Aluminium lap shear, room temperature 20.7 MPa Cohesive failure reported.
Galvanised-steel lap shear, room temperature 17.2 MPa Cohesive failure reported.
Aluminium hot strength at 82°C 10.3 MPa Thin-layer cohesive failure reported.
Aluminium after 500 h salt spray 18.3 MPa Tested after 24 hours; thin-layer cohesive failure reported.
Aluminium after 14 days at 38°C/100% RH 20.0 MPa Cohesive failure reported.
Applications and joint design

Use 406/19 where the accelerator choice, 4:1 equipment, and listed-system evidence match the assembly

LORD 406/19 is positioned for metals, engineered plastics, sign assemblies, enclosures, heavy-duty trucks, trailers, and vehicle accessories. The sign-industry application guide specifically identifies 406/19 for cold-rolled steel, aluminium, and stainless steel and references UL files E225855 and MH26317. Final qualification must address substrate lot and finish, thermal-expansion mismatch, joint geometry, bondline, impact, peel, corrosion, weathering, post-bake exposure, dimensional movement, and failure mode.

Product resources

406/19 technical, processing, and application guidance

Technical Data Sheet — DS3882

Controlling product-family TDS containing the 406/19 mix ratio, processing times, cured properties, bond data, and environmental results.

Open resource
LORD 400 Series Acrylics User Instructions — UI3031

Cartridge levelling, mixer attachment, purging, bead application, mating, fixturing, cleanup, and storage guidance.

Open resource
Powder Coating after Bonding — TT3068

Post-bake design guidance for LORD acrylic adhesive assemblies, including temporary softening and fixture support.

Open resource
Structural Adhesive Bonding Application Guide — AG1018

Joint design, surface preparation, failure-mode, cartridge, bondline, fixturing, and rework guidance.

Open resource
LORD Structural Adhesives Selector Guide — SG1018

General product-selection and market-positioning guidance.

Open resource
Sign Industry Application Guide — AG1021

Product-specific sign-assembly context and UL file references for LORD 406/19.

Open resource

Validate the LORD® 406/19 system for your structural assembly

Krayden can help review substrate preparation, 4:1 package and equipment configuration, static mixer, purge, bead size, work time, fixturing, bondline control, UL construction, environmental exposure, powder-coat processing, and final assembly qualification.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers