LORD 406

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LORD 406

Main features

  • Medium-Work-Time Acrylic Adhesive
  • 6 to 10-Minute Working Window
  • 18.6 MPa Cured Tensile Strength

Product Description

LORD® 406 Acrylic Adhesive is a two-component structural acrylic adhesive used with LORD Accelerator 17, 19, 19 Black, 19GB, or 19GB Grey. It bonds a wide range of prepared or minimally prepared metals and engineered thermoplastics and is formulated for high impact and peel performance in room-temperature-cured assemblies. LORD 406 provides a typical 6–10 minute working time at 24°C, 12–17 minute handling-strength time, and 24-hour full cure. With LORD Accelerator 19, typical cured properties include 18.6 MPa tensile strength, 30% elongation, 896 MPa Young’s modulus, and 72°C glass-transition temperature.

Key features

  • Medium-working-time structural acrylic adhesive for metals and engineered plastics
  • Non-sag paste for vertical or overhead application
  • High impact and peel performance, including low-temperature environments
  • Multiple accelerator options for 10:1 or 4:1 volumetric processing
  • Accelerator 19 improves high-temperature resistance
  • Accelerator 19GB contains glass beads for controlled bondline thickness
  • UL 746C positioning when used with LORD Accelerator 19, subject to the current listed construction

Applications

  • Bare, galvanised, and powder-coated metal assemblies
  • Engineered thermoplastics including polycarbonate, ABS, acrylic, and validated blends
  • Truck, trailer, vehicle-accessory, sign, enclosure, and equipment assembly
  • Bonded assemblies that undergo a validated e-coat or powder-coat bake

Technical Specifications

General Properties
Color
The color
Off-White to Tan Paste
Density
Volumetric mass per unit
1090 -1162 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
15 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
100000 to 300000 mPa.s

Additional Information

Medium-work-time structural acrylic adhesive

LORD® 406 Acrylic Adhesive

A two-component, non-sag acrylic adhesive used with LORD Accelerator 17, 19, 19 Black, 19GB, or 19GB Grey. The system bonds many prepared or minimally prepared metals and engineered thermoplastics and is formulated for high impact and peel strength in room-temperature-cured structural assemblies.

Structural acrylicNon-sag6–10 min work time12–17 min handling-40°C to 149°C positioning
LORD 406 acrylic adhesive
As supplied and mixed

Off-white-to-tan adhesive paste with accelerator-specific ratios

Property Published value Context
Adhesive appearance Off-white to tan paste LORD 406 component.
Viscosity at 25°C 100,000–300,000 cP Brookfield; typical, not a specification limit.
Density 1090–1162 kg/m³ LORD 406 component.
Flash point 15°C Refer to current SDS and label for safe handling.
Mix ratio with Accelerator 17 10:1 by volume; 9.33:1 by weight Adhesive to accelerator.
Mix ratio with Accelerator 19 or 19 Black 4:1 by volume; 3.02:1 or 3.00:1 by weight Accelerator 19 improves high-temperature resistance.
Mix ratio with Accelerator 19GB or 19GB Grey 4:1 by volume; 2.91:1 or 2.85:1 by weight Glass beads support bondline control.
Solids content 100% Mixed system.
Mixed appearance Tan, grey, or black paste depending on accelerator Even colour distribution indicates thorough mixing.
Preparation, mixing, and application

Remove loose contamination, maintain ratio control, and apply within the working window

  • Remove grease, loose contamination, and poorly adhering oxides from metal surfaces.
  • Normal mill oils and drawing compounds may be tolerated, but production surfaces must be tested.
  • Clean engineered plastics and abrade only where required for optimum performance.
  • Level cartridge plungers before attaching the mixer and discard the initial purge until colour is uniform.
  • Use the correct static mixer and accelerator-specific package ratio.
  • Apply with handheld cartridges or automatic meter/mix/dispense equipment.
  • Mate parts before the 6–10 minute working time expires and avoid trapping air.
  • Design joints for shear or compression and minimise peel or cleavage loading.
LORD 406 and cartridge
Cure, fixturing, and powder coating

Reach handling strength before movement or post-bake exposure

Working time

6–10 minutes at 24°C. Higher temperature shortens the usable window.

Handling strength

12–17 minutes at 24°C, based on the TDS 60 psi shear criterion.

Full cure

24 hours at 24°C under the published TDS condition.

Powder coating

LORD 406/19GB has documented post-bake resistance to 204°C for 90 minutes. Support fixtures may be required while heated adhesive temporarily softens.

Storage and industrial safety

LORD 406 is a flammable acrylic adhesive component with a published 15°C flash point. The supplied EHS identifier could not be verified as a readable product-specific safety document. Before publication and use, confirm the current regional LORD 406 SDS and the SDS for the selected Accelerator 17, 19, 19 Black, 19GB, or 19GB Grey. Follow all label controls for ventilation, ignition sources, personal protection, spill response, storage, transport, and disposal.

Cured properties and bond performance

Tough cured acrylic with substrate- and environment-specific joint results

Typical cured-property values below apply to LORD 406 mixed with Accelerator 19. Bond results are tied to the documented substrates, surface conditions, specimen geometry, cure, and test environment.

Property or joint Typical result Context
Tensile strength at break 18.6 MPa Modified ASTM D638; LORD 406/Accelerator 19.
Elongation 30% Modified ASTM D638.
Young’s modulus 896.3 MPa Modified ASTM D638.
Glass-transition temperature 72°C ASTM E1640 by DMA.
Aluminium lap shear, room temperature 20.7 MPa Cohesive failure reported.
Galvanised-steel lap shear, room temperature 17.2 MPa Cohesive failure reported.
Aluminium hot strength at 82°C 10.3 MPa Thin-layer cohesive failure reported.
Aluminium after 500 h salt spray 18.3 MPa Tested after 24 hours; thin-layer cohesive failure reported.
Aluminium after 14 days at 38°C/100% RH 20.0 MPa Cohesive failure reported.
Applications and joint design

Replace selected mechanical fasteners only after validating the complete bonded assembly

The TDS positions LORD 406 as an alternative to welding, brazing, riveting, and other mechanical fastening methods. Selector guides place the product in heavy-duty truck, service-truck, trailer, vehicle-accessory, sign, enclosure, and general industrial assembly. Final qualification should address substrate lot and coating, joint geometry, bondline, accelerator choice, cure temperature, impact, peel, fatigue, corrosion, weathering, post-bake exposure, dimensional movement, and failure mode.

Product resources

Technical, processing, and market-selection guidance

TDS DS3882

Official Parker LORD resource supporting product selection, processing, joint design, or application context.

Open resource
UI3031

Official Parker LORD resource supporting product selection, processing, joint design, or application context.

Open resource
TT3068

Official Parker LORD resource supporting product selection, processing, joint design, or application context.

Open resource
AG1018

Official Parker LORD resource supporting product selection, processing, joint design, or application context.

Open resource
SG1018

Official Parker LORD resource supporting product selection, processing, joint design, or application context.

Open resource
SG1031

Official Parker LORD resource supporting product selection, processing, joint design, or application context.

Open resource
SG1030

Official Parker LORD resource supporting product selection, processing, joint design, or application context.

Open resource

Validate LORD® 406 and the selected accelerator for your assembly process

Krayden can help review substrate preparation, accelerator selection, package ratio, static mixer, purge, bead size, bondline control, work time, fixturing, environmental exposure, e-coat or powder-coat bake, and assembly qualification.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers