LORD 403/19

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 403/19

Main features

  • 2 to 4-Minute Working Window
  • Impact-Resistant Acrylic Bonding
  • Non-Sag Placement Control

Product Description

LORD® 403 Acrylic Adhesive with LORD® Accelerator 19 Black is a two-component structural acrylic adhesive system designed to bond a wide range of prepared or unprepared metals and engineered plastics. The non-sag formulation remains in position on vertical and overhead surfaces and provides high impact and peel strength for assemblies exposed to low temperatures, environmental conditions and demanding mechanical loads. LORD Accelerator 19 improves high-temperature resistance and produces a black cured adhesive system.

Key Features

  • Fast room-temperature processing with a 2–4 minute working time and handling strength in 4–6 minutes at 75°F (24°C).
  • Broad substrate capability for unprepared metals and engineered thermoplastics, including polycarbonate, ABS and acrylics.
  • Non-sag application supports vertical and overhead bonding while maintaining placement.
  • Environmental and temperature resistance from -40°F to 300°F (-40°C to 149°C), with resistance to moisture, salt spray, weathering and indirect UV exposure.

Applications / Suitable for

  • Structural bonding of prepared or unprepared metals
  • Engineered thermoplastic assemblies
  • Vertical and overhead bonding applications
  • Assemblies exposed to high impact or peel loads

Technical Specifications

General Properties
Color
The color
Off-White to Tan Paste
Density
Volumetric mass per unit
1144 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
15 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
100000 to 300000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed-system properties for LORD® 403 Acrylic Adhesive used with LORD® Accelerator 19 Black. Values are typical and are not intended for specification purposes.

Property LORD 403 Adhesive Accelerator 19 Black Mixed System Method / Condition
Appearance Off-white to tan paste Black/gray paste Gray paste Typical
Viscosity 100,000–300,000 cP ≥250,000 mPa·s — LORD 403: Brookfield at 77°F (25°C); Accelerator 19 Black: 25°C
Density 9.25–9.55 lb/gal
(1108–1144 kg/m³)
12.55 lb/gal
(1.51 g/cm³)
— Typical
Flash Point 59°F
(15°C)
≥201°F
(≥93°C)
— Setaflash closed cup
Mix Ratio 4 parts by volume
3.00 parts by weight
1 part 4:1 by volume
3.00:1 by weight
Adhesive to Accelerator 19 Black
Solids Content — — 100% Mixed adhesive system
Working Time — — 2–4 minutes At 75°F (24°C)
Time to Handling Strength — — 4–6 minutes At 75°F (24°C); 50 psi shear
Typical Shelf Life 9 months — — Below 80°F (27°C) in original, unopened container; storage at 40–50°F (4–10°C) recommended
Technical Properties

After-Processing / Final-State Properties

Typical cured properties for LORD® 403 Acrylic Adhesive mixed with LORD® Accelerator 19. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Full Cure Time 24 hours At 75°F (24°C); approximately 90% of full strength after 2 hours
Cured Appearance Black — With Accelerator 19 Black
Tensile Strength at Break 2700
(18.6)
psi
(MPa)
ASTM D638, modified; LORD 403 with Accelerator 19
Elongation 30 % ASTM D638, modified; LORD 403 with Accelerator 19
Young’s Modulus 130,000
(896.3)
psi
(MPa)
ASTM D638, modified; LORD 403 with Accelerator 19
Glass Transition Temperature 162
(72)
°F
(°C)
ASTM E1640-99, by DMA; LORD 403 with Accelerator 19
Temperature Range -40 to 300
(-40 to 149)
°F
(°C)
Documented product-family performance range