LORD 320/322

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 320/322

Main features

  • Primerless Automotive-SMC Adhesion
  • -40 to 204 deg C Service Range
  • Solvent-Free Nonflammable Epoxy

Product Description

LORD® 320/322 Epoxy Adhesive is a general-purpose, two-component epoxy adhesive formulated for primerless adhesion to automotive sheet molded compounds (SMC). It also provides excellent adhesion to prepared metals, rubber, fiberglass reinforced plastics, polyester thermosets, thermoplastics and other supported materials. The solvent-free system can be cured at room temperature or with heat for faster processing and provides durable performance across mixed-stress, high-temperature shear and low-temperature peel joint designs.

Key Features

  • Primerless adhesion to automotive SMC with documented bonding to prepared metals, rubber, FRP, polyester thermosets and thermoplastics.
  • Durable structural performance with impact resistance down to -40°F (-40°C) and resistance to humidity, sunlight, salt spray and temperature extremes.
  • High-temperature process resistance supporting postbake exposure up to 400°F (204°C).
  • Solvent-free formulation that is nonflammable and virtually odorless.

Applications / Suitable for

  • Automotive sheet molded compound bonding
  • Prepared metal and composite assemblies
  • Fiberglass reinforced plastic, polyester thermoset and thermoplastic bonding
  • Prepared natural rubber and styrene-butadiene rubber bonding

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
320 Resin: Off White Paste | 322 Hardener: Grey Paste
Density
Volumetric mass per unit
Resin: 1498 -1546 | Hardener: 1238 -1263 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
Resin: 300,000 -1,000,000 | Hardener: 450,000 -2,000,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
Resin: >93 | Hardener: >93 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed properties. Values are typical and are not intended for specification purposes.

Property 320 Resin 322 Hardener Mixed Method / Condition
Appearance Off-white paste Grey paste Grey paste Typical
Viscosity 300,000–1,000,000 cP 450,000–2,000,000 cP — Brookfield HBF, Helipath, 5 rpm at 77°F (25°C); T-Bar D for resin and T-Bar E for hardener
Density 12.5–12.9 lb/gal
(1498–1546 kg/m³)
10.33–10.54 lb/gal
(1238–1263 kg/m³)
— Typical
Flash Point >200°F
(>93°C)
>200°F
(>93°C)
— Closed cup
General-Purpose Mix Ratio 1 part 1 part by volume
0.83 part by weight
1:1 by volume
1.2:1 by weight
Mixed-stress joint design; -40°F to 400°F (-40°C to 204°C)
High-Temperature Mix Ratio 1.5 parts by volume
1.8 parts by weight
1 part 1.5:1 by volume
1.8:1 by weight
Shear-stress joint design; 50°F to 400°F (10°C to 204°C)
Low-Temperature Mix Ratio 1 part 1.5 parts by volume
1.2 parts by weight
1:1.5 by volume
1:1.2 by weight
Peel-stress joint design; -40°F to 100°F (-40°C to 38°C)
Solids Content — — 100% Mixed adhesive
Working Time — — 20–40 minutes 54 g mass at 75°F (24°C)
Time to Handling Strength — — 2–4 hours Typical
Recommended Film Thickness — — 0.02–0.03 in
(0.51–0.76 mm)
General use
Shelf Life 2 years 2 years — From date of manufacture; store at 60–80°F (16–27°C) in original, unopened containers
Technical Properties

After-Processing / Final-State Properties

Typical cured properties. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Cure to Full Strength Approximately 24 hours Adhesive, substrates and ambient temperature at 65°F (18°C) or higher
Accelerated Cure 45–60 minutes At 180°F (82°C); bondline temperature should not exceed 325°F (162°C)
Cured Appearance Grey — Typical
Tensile Strength at Break 4440
(30.6)
psi
(MPa)
ASTM D882-83A, modified
Elongation 3 % ASTM D882-83A, modified
Young’s Modulus 230,000
(1586)
psi
(MPa)
ASTM D882-83A, modified
Glass Transition Temperature (Tg) 176
(80)
°F
(°C)
ASTM E1640-99, by DMA
Cold-Rolled Steel Lap Shear Strength 2225
(15.3)
psi
(MPa)
Room temperature; 72-hour room-temperature cure; 1:1 mix ratio by volume
Aluminum Lap Shear Strength 1690
(11.7)
psi
(MPa)
Room temperature; 72-hour room-temperature cure; 1:1 mix ratio by volume
SMC Lap Shear Strength 620
(4.3)
psi
(MPa)
Room temperature; 72-hour room-temperature cure; 1:1 mix ratio by volume; fiber-tear failure mode
Cold-Rolled Steel Lap Shear after Salt Spray 2260
(15.6)
psi
(MPa)
Tested immediately after 14 days of salt-spray exposure
SMC Lap Shear at -30°F (-34°C) 731
(5.0)
psi
(MPa)
Fiber-tear failure mode

 

Leading Brands Trust in Our Products and Services