LORD 3170

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LORD 3170

Main features

  • Bond Strength Down to -253 deg C
  • Low-Outgassing Aerospace Epoxy
  • Equal-Volume Room-Temperature Cure

Product Description

LORD® 3170-A/3170-B Epoxy Adhesive is an equal-mix, two-component epoxy structural adhesive designed to bond metals, glass, reinforced plastics, ceramics and foam materials in cryogenic applications. The system provides high bond strength at very low temperatures and minimal outgassing for aerospace use. It can be cured at room temperature or with elevated heat for faster processing and improved mechanical properties and bond strength.

Key Features

  • Cryogenic performance with documented tensile shear and butt tensile strength at temperatures down to -423°F (-253°C).
  • Minimal outgassing with 1.47% total mass loss and 0.02% collected volatile condensable materials per ASTM E595-84.
  • Equal-volume mixing of 3170-A resin and 3170-B hardener for straightforward manual or cartridge application.
  • Room-temperature or accelerated curing with improved mechanical properties and bond strength following a 1-hour postbake at 212°F (100°C).

Applications / Suitable for

  • Cryogenic structural bonding
  • Aerospace assemblies requiring minimal outgassing
  • Bonding metals, glass, reinforced plastics and ceramics
  • Bonding foam insulation materials to solid substrates

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
3170A Resin: Milky White Liq | 3170B Hardener: Amber Liq
Density
Volumetric mass per unit
Resin: 1138 | Hardener: 971 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
Resin: 55000 | Hardener: 130000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
Resin: >93 | Hardener: >93 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed properties. Values are typical and are not intended for specification purposes.

Property 3170-A Resin 3170-B Hardener Mixed Method / Condition
Appearance Milky white liquid Amber liquid Light amber paste Typical
Viscosity 55,000 cP 130,000 cP — At 77°F (25°C)
Density 9.55 lb/gal
(1138 kg/m³)
8.1 lb/gal
(971 kg/m³)
— Typical
Flash Point >201°F
(>93°C)
>201°F
(>93°C)
— Setaflash closed cup
Mix Ratio 1 part 1 part 1:1 Resin to hardener, by volume
Solids Content — — 100% Mixed adhesive
Working Time — — 2 hours At 75°F (24°C)
Time to Handling Strength — — 24 hours Typical
Recommended Film Thickness — — 0.002–0.003 in
(0.05–0.07 mm)
General use
Recommended Film Thickness — — 0.01 in
(0.25 mm)
Foam insulation bonded to solid substrates
Shelf Life 2 years 2 years — From date of manufacture; store at 60–80°F (16–27°C) in original, unopened containers
Technical Properties

After-Processing / Final-State Properties

Typical cured properties. Unless otherwise stated, cured-property and bond-performance data were generated after 24 hours at room temperature followed by 1 hour at 149°F (65°C) under 10 psi pressure.

Property Value Unit Method / Condition
Cure to Full Strength 4 days At 75°F (24°C)
Recommended Postbake 1 hour — At 212°F (100°C); improves mechanical properties and bond strength
Cured Appearance Yellow to honey-colored — Typical
Hardness 70 Shore D Typical
Coefficient of Linear Thermal Expansion 3 × 10-5 in/in/°F From -423°F to 32°F (-253°C to 0°C)
Total Mass Loss 1.47 % ASTM E595-84
Collected Volatile Condensable Materials 0.02 % ASTM E595-84
Tensile Shear Strength 2500
(17.2)
psi
(MPa)
At -423°F (-253°C); 7075-T6 bare aluminum alloy, tested per MIL-A-5090D
Tensile Shear Strength 3000
(20.7)
psi
(MPa)
At room temperature; 7075-T6 bare aluminum alloy, tested per MIL-A-5090D
Butt Tensile Strength 5800
(40.0)
psi
(MPa)
At -423°F (-253°C); Federal Test Method Standard 175, Methods 1051 and 1051.1T
Lap Shear Strength after Humidity Exposure 2500
(17.2)
psi
(MPa)
At room temperature after 720 hours at 100% RH and 165°F (74°C)
Lap Shear Strength after Salt Spray Exposure 2900
(20.0)
psi
(MPa)
At room temperature; saturated salt spray exposure per MIL-A-005090C and Federal Test Standard 51

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers