LORD 3135-B

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 3135-B

Main features

  • Former Lord 7111-B Hardener
  • Low-Shrinkage Epoxy Bonding
  • Room-Temperature or Accelerated Heat Curing

Product Description

LORD® 7111-B is the former designation for the hardener now identified as LORD® 3135-B. When mixed in equal parts by weight with LORD® 3135-A resin, it forms a two-component structural epoxy adhesive for bonding metals, wood, glass, concrete, masonry and supported synthetic materials. The mixed system is especially suited to bonding skins to plastic or metal honeycomb cores, polyurethane foams, and phenolic or epoxy laminates, with room-temperature and accelerated heat-cure options.

Key Features

  • Former LORD® 7111-B designation corresponds to the LORD® 3135-B hardener used with LORD® 3135-A resin.
  • Equal-weight mixing with LORD® 3135-A resin produces a 100% solids structural epoxy adhesive.
  • Low-stress cured system provides low cure shrinkage, bondline flexibility and good electrical resistance.
  • Qualified mixed-system performance meets NASA Low Outgassing Specification, MMM-A-134 Types 1 and 2, and MIL-A-8623A Types 1 and 2 requirements.

Applications / Suitable for

  • Use with LORD® 3135-A resin in structural adhesive systems
  • Bonding skins to plastic or metal honeycomb cores
  • Polyurethane foam bonding
  • Phenolic and epoxy laminate bonding
Product Family

LORD 3135-B

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber Liquid
Density (g)
0.96 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
25,000 - 50,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>93 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical properties for LORD® 7111-B, now designated LORD® 3135-B, and supported processing properties of the mixed LORD® 3135-A/B adhesive system.

Property Value Unit Method / Condition
Current Designation LORD® 3135-B Hardener — Formerly LORD® 7111-B
Appearance Amber liquid — Typical, as supplied
Viscosity 25,000–50,000 cP Brookfield at 77°F (25°C)
Density 8.01
(0.96)
lb/gal
(g/cm³)
Typical
Flash Point ≥201
(≥93)
°F
(°C)
Closed cup
Mix Ratio with LORD® 3135-A Resin 1:1 by weight Resin to hardener
Recommended Induction Period 15 minutes After mixing and before application
Solids Content 100 % Mixed LORD® 3135-A/B system
Working Time 1.5–3 hours Mixed system at 77°F (25°C)
Time to Handling Strength 8–12 hours Mixed system
Mixed Appearance Straw-yellow liquid — LORD® 3135-A resin with LORD® 7111-B / 3135-B hardener
Shelf Life 2 years Store at 73°F (23°C) in a clean, dry environment in the original, unopened container
Technical Properties

After-Processing / Final-State Properties

Typical cured-system properties for LORD® 3135-A resin mixed with LORD® 7111-B, now designated LORD® 3135-B hardener.

Property Value Unit Method / Condition
Full Cure Time Approximately 24 hours At 77°F (25°C)
Accelerated Cure 45 minutes
1 hour
3 hours
— At 121°C
At 93°C
At 65°C
Cured Appearance Amber to clear — Typical
Volume Resistivity 1.25 × 1014 ohm/cm ASTM D257-252T
Coefficient of Linear Thermal Expansion 57.6 ppm/°C Typical
Hardness 82 Shore D Typical
Dielectric Strength 460 V/mil ASTM D149-44; 60 cycles at room temperature
Dielectric Constant 3.24 — ASTM D159-47T; 60 cycles at room temperature
Arc Resistance 78 seconds ASTM D495-48T
Lap Shear Strength 3800
(26.2)
psi
(MPa)
2024-T3 clad aluminum at 75°F (24°C)