LORD 310

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 310

Main features

  • Thixotropic Application Control
  • 30 to 60-Minute Working Window
  • 32 MPa Cured Tensile Strength

Product Description

LORD® 310 Epoxy Adhesive is a modified, thixotropic two-component epoxy adhesive for bonding prepared metals, rubber, urethane, plastics, glass, and ceramics under the documented preparation conditions. The solvent-free system may be cured at room temperature or with heat and has a typical working time of 30 to 60 minutes at 24°C. Supported applications include disk drives, down-hole oil-field equipment, automotive body panels and spoilers, sheet-molded compound, and vibration-damping mounts. Typical cured properties include 32 MPa tensile strength, 60°C glass-transition temperature, and service from -40°C to 204°C.

Key features

  • Thixotropic two-part epoxy: The paste system supports controlled application to prepared substrates.
  • Room-temperature or heat cure: Typical working time is 30 to 60 minutes at 24°C, with full strength in 24 hours at 18°C or higher.
  • Broad temperature range: The documented service-temperature range is -40°C to 204°C.

Applications / Suitable for

  • Disk drives and down-hole oil-field equipment
  • Automotive body panels and spoilers
  • Sheet-molded compound and vibration-damping mounts

Technical Specifications

General Properties
Color
The color
Off-white Paste / Black Paste
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Resin/Hardener)
Density (g)
1.402-1.540 / 1.234-1.318 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Appearance, 310-A resin Off-white paste N/A As supplied
Appearance, 310-B hardener Gray paste N/A As supplied
Viscosity, 310-A 400,000 to 820,000 cP Brookfield HBF, Helipath T-C spindle, 5 rpm at 25°C
Viscosity, 310-B 230,000 to 690,000 cP Brookfield HBF, Helipath T-C spindle, 5 rpm at 25°C
General-purpose mix ratio 1:1 parts by volume Resin : hardener
Working time 30 to 60 min 54 g mass at 24°C
Time to handling strength 6 to 8 h Typical mixed system
Full cure 24 h At 18°C or higher
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Tensile strength 32 MPa ASTM D882-83A, modified
Elongation 2 % ASTM D882-83A, modified
Young's modulus 1,689 MPa ASTM D882-83A, modified
Glass-transition temperature 60 °C ASTM E1640-99 by DMA
Service temperature -40 to 204 °C Documented range

Leading Brands Trust in Our Products and Services