LORD 309-1D

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LORD 309-1D

Main features

  • Non-Sag Vertical Bonding
  • 1.5-2 Hour Work Time
  • Room- or Heat-Cure Flexibility

Product Description

LORD 309-1D Epoxy Adhesive Component is the blue, thixotropic epoxy resin component used with LORD 309-2D hardener in two-part structural adhesive systems. The resin supports gap filling and non-sag application on vertical surfaces for prepared metals, FRP, wood, and prepared rubber. Mixed-system ratios vary with joint design, while a 54 g mass provides a typical 1.5 to 2 hour working time at 24 deg C and 8 to 16 hours to handling strength. The cured 309-1D/309-2D system develops 37.9 MPa tensile strength, 6% elongation, and a 70 deg C glass transition temperature.

Key features

  • Thixotropic Gap Filling: Supports non-sag application on vertical surfaces and gap-filling bondlines.
  • Extended Working Time: Provides 1.5 to 2 hours of working time for a 54 g mixed mass at 24 deg C.
  • Room- or Heat-Cure Processing: The complete system can cure at room temperature or with applied heat.

Applications

Applications include structural bonding of prepared metals, FRP, wood, and prepared rubber where gap filling or vertical-surface application is required.

Technical Specifications

General Properties
Color
The color
Blue Paste
Density
Volumetric mass per unit
1258 - 1294 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>93 °C

Additional Information

Technical properties

Resin component properties

Values apply to LORD 309-1D resin before mixing with LORD 309-2D hardener.

Property Value Unit Method / condition
Appearance Blue paste LORD 309-1D resin
Viscosity 300,000 to 1,100,000 mPa s 25 deg C
Density 10.5 to 10.8 lb/gal 25 deg C
Flash point >93 deg C Closed-cup value
Technical properties

309-1D / 309-2D system properties

System values require LORD 309-2D hardener; the supplier specifies different mix ratios for different joint designs.

Property Value Unit Method / condition
Working time 1.5 to 2 h 54 g mixed mass at 24 deg C
Handling-strength time 8 to 16 h Room-temperature cure
Full-strength development 24 h Bondline maintained at or above 18 deg C
Tensile strength 37.9 MPa Cured 309-1D / 309-2D system
Elongation at break 6 % Cured 309-1D / 309-2D system
Glass transition temperature 70 deg C Cured 309-1D / 309-2D system
Service temperature range -34 to 121 deg C Complete bonded system