LORD 306-1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 306-1

Main features

  • High-Viscosity Non-Sag Gap Filling
  • Documented Chemical/Moisture/Weather Resistance
  • MIL-A-24456 Compliance Scope

Product Description

LORD® 306-1/306-2 Epoxy Adhesive is a general-purpose, high-viscosity, two-component epoxy adhesive formulated for structural bonding applications requiring excellent gap-filling capability and non-sag performance on vertical or overhead surfaces. The adhesive system provides durable, chemically and environmentally resistant bonds and conforms to MIL-A-24456 for bonding plastic vibration damping tiles to steel. It can be cured at room temperature or heat cured for faster production while delivering reliable service across temperatures from -30°F to +250°F (-34°C to +121°C). :contentReference[oaicite:0]{index=0}

Key Features

  • High-viscosity, non-sag epoxy formulation for gap filling and vertical or overhead applications.
  • Provides durable structural bonds with resistance to moisture, weathering, dilute acids, alkalis, solvents, greases and oils.
  • Low-shrinkage adhesive with good creep resistance and low water absorption for demanding industrial assemblies.

Applications / Suitable for

  • General structural bonding applications
  • Gap-filling and non-sag bonding on vertical or overhead surfaces
  • Bonding plastic vibration damping tiles to steel
  • Industrial metal and engineering material assemblies

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
306-1 Resin: Grey Paste | 306-2 Hardener: Off White Paste
Density
Volumetric mass per unit
Resin: 1378 -1474 | Hardener: 1007-1078 kg/m3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
Resin: 40,000 - 400,000 | Hardener: 20,000 - 100,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
Resin: 85 | Hardener: >93 °C

Additional Information

As-Supplied / Before-Processing Properties

Property 306-1 Resin 306-2 Hardener Method / Condition
Appearance Grey Paste Off-white Paste Typical
Viscosity 40,000–400,000 P 20,000–100,000 P Brookfield HBF, Helipath, 1 rpm (T-Bar Spindle E / C), 77°F (25°C)
Density 11.5–12.3 lb/gal (1378–1474 kg/m³) 8.4–9.0 lb/gal (1007–1078 kg/m³) Typical
Flash Point 185°F (85°C) >200°F (>93°C) Closed Cup
General Purpose Mix Ratio 1:1.3 by volume (1:1 by weight) -30°F to +250°F (-34°C to +121°C)
MIL-A-24456 Mix Ratio 5:3 by weight Specification
Solids Content 100% Mixed adhesive
Working Time 1–2 hours 75°F (24°C), 54 g mass
Time to Handling Strength 8–16 hours Temperature dependent
Mixed Appearance Grey Paste Typical
Shelf Life 2 years Stored unopened at 60–80°F (16–27°C)

After-Processing / Final-State Properties

Property Value Method / Condition
Cure Schedule 24–48 hours 65°F (18°C) or higher
Service Temperature -30°F to +250°F (-34°C to +121°C) Typical operating range
Tensile Strength at Break 4360 psi (30.1 MPa) ASTM D882-83A (modified)
Elongation 10% ASTM D882-83A (modified)
Young's Modulus 146,070 psi (1007 MPa) ASTM D882-83A (modified)
Glass Transition Temperature (Tg) 133°F (56°C) ASTM E1640-99 by DMA
Cured Appearance Grey Typical

Leading Brands Trust in Our Products and Services