LORD 2850

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 2850

Main features

  • 62.1 MPa Compressive Strength
  • Low-Outgassing 0.01% CVCM
  • Trowel or Injection Application

Product Description

LORD® 2850-A/2850-B Syntactic Foam is a two-component modified epoxy syntactic foam with a smooth, creamy consistency suited to trowel and injection application. The mixed material forms a green, thixotropic paste used to reinforce honeycomb cores and other hollow structures. After cure, it combines high compressive strength with low weight relative to volume and supports service temperatures from -320°F to 225°F (-196°C to 107°C).

Key Features

  • High cured compressive strength of 9000 psi (62.1 MPa) at room temperature and 12,000 psi (82.7 MPa) at -320°F (-196°C).
  • Low-outgassing cured performance with 0.98% total mass loss and 0.01% collected volatile condensable materials per ASTM E595.
  • Application-friendly mixed consistency suitable for injection or spatula application, with a 30-minute working time at 77°F (25°C).

Applications / Suitable for

  • Reinforcement of honeycomb cores
  • Reinforcement of hollow structures
  • Aerospace structures requiring low-outgassing syntactic foam
Product Family

LORD 2850

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
A: Yellow Paste | B: Blue Liquid | Mixed: Green Paste
Density
Volumetric mass per unit
A: 600-695 | B: 940-1000 | Mixed: 640-700 kg/m3
Physical Properties
Viscosity (Part A)
(Thixotropic) mPa.s
Viscosity (Part B)
50 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
A/B/Mixed: >125 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed properties. Values are typical and are not intended for specification purposes.

Property 2850-A Component 2850-B Component Mixed Method / Condition
Appearance Yellow paste Blue liquid Green paste Typical
Viscosity Thixotropic 50 cP Thixotropic Typical
Density 5.0–5.8 lb/gal
(600–695 kg/m³)
7.8–8.3 lb/gal
(940–1000 kg/m³)
5.3–5.8 lb/gal
(640–700 kg/m³)
Typical
Flash Point >257°F
(>125°C)
>257°F
(>125°C)
>257°F
(>125°C)
Typical
Mix Ratio 100 parts 8 parts 100:8 By weight; thoroughly stir 2850-B before mixing
Working Time — — 30 minutes At 77°F (25°C)
Time to Handling Strength — — 1 hour Typical
Shelf Life 6 months 6 months — Store at 68–86°F (20–30°C) in a clean, dry environment in original, unopened containers
Technical Properties

After-Processing / Final-State Properties

Typical cured properties. The recommended cure is 24 hours at 77–86°F (25–30°C). Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Compressive Strength 9000
(62.1)
psi
(MPa)
At room temperature
Compressive Strength 12,000
(82.7)
psi
(MPa)
At -320°F (-196°C)
Tensile Shear Strength 2500
(17.2)
psi
(MPa)
At room temperature
Tensile Shear Strength 1800
(12.4)
psi
(MPa)
At -320°F (-196°C)
Total Mass Loss 0.98 % ASTM E595
Collected Volatile Condensable Materials 0.01 % ASTM E595
Service Temperature Range -320 to 225
(-196 to 107)
°F
(°C)
Documented performance range