LOCTITE SICOMET 100

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE SICOMET 100

Main features

  • 0.01 to 0.50 mm Gap Fill
  • Fast Moisture-Cure Fixturing
  • Strong Rubber/Plastic Adhesion

Product Description

LOCTITE® SICOMET 100 is a fast-curing, medium-viscosity ethyl cyanoacrylate instant adhesive designed for bonding a wide range of materials including plastics, rubbers, metals, fabrics, and foam materials. The one-component adhesive cures rapidly through surface moisture and develops handling strength within seconds on close-fitting parts. It offers excellent adhesion to plastics and elastomers while requiring no mixing, making it suitable for high-speed assembly and repair operations.

Key Features & Benefits

  • Ethyl cyanoacrylate instant adhesive technology.
  • Excellent adhesion to rubbers and plastics.
  • Fast fixture and cure speed.
  • Medium-low viscosity for easy application.
  • One-component formulation requiring no mixing.
  • Easy dispensing and handling.
  • Suitable for close-fitting assemblies.

Recommended Applications

  • Plastic component assembly.
  • Rubber and elastomer bonding.
  • Foam material bonding.
  • Metal bonding applications.
  • Fabric assembly and repair.
  • General-purpose instant bonding operations.
Product Family

LOCTITE SICOMET 100

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colorless liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.05 - 1.10
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
140 - 220 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Ethyl Cyanoacrylate — Instant adhesive
Appearance Colourless Liquid — Uncured material
Components One Part — No mixing required
Viscosity Classification Medium-Low — Product characteristic
Specific Gravity 1.05 - 1.10 — 25°C
Viscosity 140 - 220 mPa·s (cP) 25°C
Cure Mechanism Surface Moisture — Moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Recommended Gap Fill 0.01 - 0.50 mm Typical bond gap
Fixture Time (Aluminium) 5 - 10 seconds Typical cure speed
Fixture Time (Steel) 10 - 30 seconds Typical cure speed
Fixture Time (Rubber, Nitrile) 5 - 10 seconds Typical cure speed
Fixture Time (ABS) 5 - 10 seconds Typical cure speed
Fixture Time (PVC) 5 - 10 seconds Typical cure speed
Tensile Shear Strength (Steel) 17 N/mm² ISO 4587, 24 h cure
Tensile Shear Strength (Aluminum) 15 N/mm² ISO 4587, 24 h cure
Tensile Shear Strength (ABS) 8* N/mm² Substrate failure