LOCTITE SI-5970

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

LOCTITE SI-5970 LOCTITE SI-5970 LOCTITE SI-5970 LOCTITE SI-5970 LOCTITE SI-5970 LOCTITE SI-5970 LOCTITE SI-5970

Main features

  • 25-Minute Tack-Free Time
  • Oil-Resistant Flexible Gasketing
  • One-Part No-Mix Application

Product Description

LOCTITE SI 5970 Flange Sealant is a one-part, black, thixotropic alkoxy silicone flange sealant for formed-in-place gasketing on stamped metal covers and other rigid flange assemblies. The moisture-curing RTV material applies without mixing, remains in position after dispensing, and becomes tack free in 25 minutes at 23 deg C and 50% relative humidity. It combines oil resistance with movement capability for timing covers, oil sumps, and similar gasketing joints. Typical cured properties include Shore A 44 hardness, at least 200% elongation, and at least 1.5 N/mm^2 tensile strength.

Key features

  • 25-Minute Tack-Free Time: Becomes tack free within 25 minutes at 23 deg C and 50% relative humidity.
  • Oil-Resistant Flexible Seal: Supports gasketing joints that require oil resistance and movement capability.
  • One-Part Thixotropic Paste: Applies without mixing and remains in position after dispensing.

Applications

Applications include formed-in-place gaskets for stamped sheet-metal covers, timing covers, oil sumps, and similar rigid flange assemblies.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black paste
Chemistry Type
Alkoxy silicone
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
1K
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.38 to 1.44
Physical Properties
Extrusion Rate
40 to 80 g/min
Tack-Free Time
25 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
≥200 %
Electrical Properties
Surface Resistivity
1.4×10^16 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.8×10^15 Ohms⋅cm

Additional Information

Technical properties

As-supplied properties

Property Value Unit Method / condition
Appearance Black paste As supplied
Component count One No mixing required
Specific gravity 1.38 to 1.44 25 deg C
Extrusion rate 40 to 80 g/min 0.62 MPa, 15 seconds, 25 deg C, Semco cartridge
Technical properties

Cured sealant properties

Values are typical for the moisture-cured sealant under the listed conditions.

Property Value Unit Method / condition
Tack-free time Within 25 min 23 +/- 2 deg C, 50 +/- 5% relative humidity
Hardness 44 Shore A ISO 868
Elongation at break >=200 % ISO 37
Tensile strength >=1.5 N/mm^2 ISO 37