LOCTITE SI 593

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

LOCTITE SI 593

Main features

  • Non-Slumping Sealant Formulation
  • Adhesion and Flexibility
  • Seals Out Moisture and Contaminants

Product Description

LOCTITE® SI 593™ BLACK is a one-component, room-temperature vulcanizing (RTV) acetoxy silicone sealant designed to provide durable sealing and bonding for a wide variety of mechanical assemblies. Upon exposure to atmospheric moisture, it cures to form a tough, flexible silicone rubber seal that resists aging, weathering, UV exposure, ozone, and thermal cycling without hardening, shrinking, or cracking. The product offers superior adhesion and flexibility and is suitable for electrical insulation, trim bonding, and sealing of ducts, vents, flues, doors, and windows.

Key Features & Benefits

  • One-component RTV acetoxy silicone sealant.
  • Non-slumping thixotropic formulation.
  • Superior adhesion and flexibility.
  • Seals out moisture and contaminants.
  • Fills large cracks and seams.
  • Resists UV, ozone, weathering and thermal cycling.
  • Non-flammable and non-toxic.
  • UL 94HB classified at 1.9 mm cross section.

Recommended Applications

  • Electrical insulation.
  • Protection of leads from mechanical shock.
  • Trim bonding applications.
  • Sealing ducts, vents and flues.
  • Sealing doors and windows.
  • General-purpose mechanical assembly sealing.
Product Family

LOCTITE SI 593

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.01

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — RTV sealant
Chemical Type Acetoxy Silicone — Moisture-curing silicone
Appearance Black — Uncured material
Components One Component — No mixing required
Viscosity Thixotropic Paste — Non-slumping
Odor Acetic Acid — Characteristic cure odor
Specific Gravity 1.01 — 25°C
Extrusion Rate ≥250 g/min Typical
Tack-Free Time ≤60 minutes Surface cure
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Full Cure Time 24 hours Moisture cure at ambient conditions
Tensile Strength ≥1.5 N/mm² ISO 37, 1 week cure
Elongation at Break ≥300 % ISO 37
Shore Hardness ≥18 Shore A ISO 868
Environmental Resistance Excellent — Resists weathering and aging
Thermal Cycling Resistance Excellent — Will not harden, shrink or crack
UV Resistance Excellent — Outdoor sealing applications
Ozone Resistance Excellent — Long-term durability

Leading Brands Trust in Our Products and Services