LOCTITE SI 5920

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI 5920

Main features

  • One-Component Sealing System
  • Non-Corrosive Sealing Formulation
  • Thixotropic Application Control

Product Description

LOCTITE® SI 5920™ is a one-component, non-corrosive RTV silicone sealant designed for gasketing and sealing applications requiring excellent temperature resistance, flexibility, and electrical insulation properties. The thixotropic formulation minimizes migration after application and provides reliable sealing on a wide range of substrates. It is commonly used in industrial and electrical applications where long-term environmental resistance and high-temperature performance are required. Based on the uploaded datasheet image.

Key Features & Benefits

  • One-component RTV silicone sealant.
  • Non-corrosive curing system.
  • Excellent temperature resistance up to 350°C service conditions.
  • Thixotropic consistency minimizes migration after application.
  • Adheres to a wide range of substrates.
  • Provides electrical insulation properties.
  • Suitable for gasketing and sealing applications.
  • Excellent environmental durability.

Recommended Applications

  • Industrial gasketing applications.
  • General-purpose sealing.
  • Electrical insulation applications.
  • High-temperature sealing systems.
  • Equipment maintenance and repair.
Product Family

LOCTITE SI 5920

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Copper colored paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.05

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — RTV sealant
Chemical Type Silicone — Non-corrosive formulation
Appearance Copper Colored Paste — Uncured material
Components One Component — No mixing required
Consistency Thixotropic — Reduced migration after application
Specific Gravity 1.05 — 22°C
Extrusion Rate ≥275 g/min 0.62 MPa, 22°C, 15 sec, Semco cartridge
Flow ≤13 mm ISO 7390, after 2 minutes
Tack-Free Time 20 - 60 minutes 25°C / 50±5% RH
Skin Over Time 20 minutes Typical
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Depth of Cure 10 mm Approximate depth after 7 days @ 22°C
Shore Hardness 23 - 38 Shore A ISO 868, cured 7 days
Elongation at Break ≥350 % ISO 37
Tensile Strength ≥1.4 N/mm² ISO 37
Coefficient of Thermal Expansion 340 × 10⁻⁶ K⁻¹ ISO 11359-2, cured 21 days
Volume Resistivity 5.5 × 10¹⁵ Ω·cm IEC 60093
Surface Resistivity 200 × 10¹⁵ Ω IEC 60093
Temperature Resistance Up to 350 °C Typical application capability

Leading Brands Trust in Our Products and Services