LOCTITE SI 5900

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI 5900

Main features

  • At Least 100-Second Blow-Out Resistance
  • At Most 0.2 mm ISO 7390 Flow
  • At Least 400% Cured Elongation

Product Description

LOCTITE SI 5900 is a one-component black oxime RTV silicone gasketing compound for stamped sheet-metal covers, including timing covers and oil sumps. The thixotropic paste has a typical specific gravity of 1.3 to 1.37 at 25 deg C. It records at least 100 seconds of blow-out resistance on a 4 mm flange with a 1.5 mm gap at 0.014 MPa and at most 0.2 mm flow after 2 minutes at 25 deg C by ISO 7390. Typical tack-free time is 7 to 24 minutes at 25 deg C and 50+/-5% RH. After one week under those conditions, cured elongation is at least 400%.

Key features

  • Flow Control: ISO 7390 flow is at most 0.2 mm after 2 minutes at 25 deg C.
  • Blow-Out Test Performance: Records at least 100 seconds on a 4 mm flange with a 1.5 mm gap at 0.014 MPa.
  • Cured Flexibility: Elongation is at least 400% by ISO 37 after one week at 25 deg C and 50+/-5% RH.

Applications

Stamped covers; timing covers; oil sumps; similar gasketing applications.

Product Family

LOCTITE SI 5900

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.3 -- 1.37
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
400 %

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
Specific gravity1.3 to 1.3725 deg C
Extrusion rate20 to 50g/min0.62 MPa for 15 seconds at 25 deg C; Semco cartridge
Blow-out resistance>=100s4 mm flange; 1.5 mm gap; 0.014 MPa
Flow<=0.2mmISO 7390; after 2 minutes at 25 deg C
Volatile content<=0.5%As reported
Technical properties

Final-state properties

PropertyValueUnitMethod / condition
Hardness31 to 46Shore AAfter 1 week at 25 deg C and 50+/-5% RH
Elongation>=400%ISO 37; after 1 week at 25 deg C and 50+/-5% RH
Tensile strength>=1.7N/mm2ISO 37; after 1 week at 25 deg C and 50+/-5% RH
Volume resistivity6.7x10^13ohm cmIEC 60093
Lap shear strength1 to 1.4N/mm2ISO 4587; mild steel; 0.5 mm gap; after 21 days at 23 deg C and 50+/-5% RH