LOCTITE SI 587

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI 587

Main features

  • 250 to 600 g/min Extrusion
  • 10 to 50 Minute Tack-Free
  • At Least 350% Cured Elongation

Product Description

LOCTITE SI 587 is a one-component metallic blue oxime RTV silicone for formed-in-place gasketing and sealing. It requires no mixing and is used for gasket replacement or dressing on assemblies including valve covers, oil pans, water pumps, intake manifolds, and rear axle housings. At 25 deg C, the uncured material has a specific gravity of 1.28 to 1.33 and a Semco-cartridge extrusion rate of 250 to 600 g/min. Tack-free time is 10 to 50 minutes at 25 deg C and 50+/-5% RH. After seven days under those conditions, cured elongation is at least 350%.

Key features

  • No-Mix Application: The one-component RTV is applied without a separate mixing step.
  • Controlled Extrusion: Typical Semco-cartridge extrusion is 250 to 600 g/min at 0.62 MPa for 15 seconds at 25 deg C.
  • Cured Flexibility: Elongation is at least 350% by ISO 37 after seven days at 25 deg C and 50+/-5% RH.

Applications

Valve covers; oil pans; water pumps; intake manifolds; rear axle housings.

Product Family

LOCTITE SI 587

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Metallic blue paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.28 0 1.33
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
350 %

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
Specific gravity1.28 to 1.3325 deg C
Extrusion rate250 to 600g/min0.62 MPa for 15 seconds at 25 deg C; Semco cartridge
Flow<=12.7mmISO 7390; after 2 minutes at 25 deg C
Technical properties

Final-state properties

Cured-property values are reported after 7 days at 25 deg C and 50+/-5% RH.

PropertyValueUnitMethod / condition
Tensile strength>=1.6N/mm2ISO 37; after 7 days at 25 deg C and 50+/-5% RH
Elongation>=350%ISO 37; after 7 days at 25 deg C and 50+/-5% RH
Hardness26 to 40Shore AISO 868; after 7 days at 25 deg C and 50+/-5% RH