LOCTITE SI 5699

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE SI 5699

Main features

  • One-Component Oxime RTV Silicone
  • Non-Corrosive Flange Sealant
  • Rigid-Flange Sealing Applications

Product Description

LOCTITE® SI 5699™ is a one-component, oxime silicone RTV sealant designed primarily for flange sealing applications. The non-corrosive, thixotropic formulation is particularly suited for rigid flange sealing on transmissions, cast metal housings, and similar industrial assemblies. It cures at room temperature to form a durable, flexible silicone gasket while offering excellent environmental resistance and minimizing material migration after application. Based on the uploaded datasheet image.

Key Features & Benefits

  • One-component RTV silicone sealant.
  • Oxime cure technology.
  • Non-corrosive formulation.
  • Designed for rigid flange sealing.
  • Thixotropic consistency minimizes migration.
  • Excellent environmental resistance.
  • NSF Category P1 registered.
  • Suitable for automotive and industrial assemblies.

Recommended Applications

  • Transmission housing sealing.
  • Cast metal housing flanges.
  • Rigid flange gasketing.
  • Industrial equipment sealing.
  • Maintenance and repair sealing operations.
Product Family

LOCTITE SI 5699

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Grey paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.45

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — RTV flange sealant
Chemical Type Oxime Silicone — Non-corrosive chemistry
Appearance Grey Paste — Uncured material
Components One Component — No mixing required
Consistency Thixotropic — Reduced migration after application
Specific Gravity 1.45 — 20°C
Extrusion Rate ≥200 g/min 0.62 MPa, 25°C, Semco cartridge
Tack-Free Time ≤30 minutes 25°C / 50±5% RH
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Shore Hardness 48 Shore A ISO 868, cured 1 week
Water Vapor Transmission Rate 5.2 g/(h·m²) Typical cured value
Water Absorption 0.87 % 24 h immersion at room temperature
Glass Transition Temperature -52 °C Typical cured value
Coefficient of Thermal Expansion 255 µm/m·K Typical cured value
Elongation at Break 230 % Typical cured value
Tensile Strength 2.8 N/mm² Typical cured value
Tear Strength 9.5 N/mm ISO 34-1
Depth of Cure 10 mm Maximum depth, PTFE mold strip
Lap Shear Strength 1.3 N/mm² ISO 4587, Aluminum substrate