LOCTITE SI 5470

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE SI 5470

Main features

  • Dual-Cure Sealing Processing
  • Low-Modulus Cured Sealing
  • Strong Plastic/Metal Adhesion

Product Description

LOCTITE® SI 5470™ is a dual-cure UV and moisture-curing silicone gasket material engineered to create soft, flexible, low-modulus foam gaskets for sealing applications. The product contains mechanically mixed nitrogen gas that produces a closed-cell foam structure and provides excellent adhesion to both plastics and metals. Functional strength develops almost instantly upon UV exposure, while secondary moisture cure ensures complete curing in shadowed areas and continued property development over 72 hours.

Key Features & Benefits

  • Dual-cure UV and moisture silicone technology.
  • Creates a closed-cell foam gasket structure.
  • Fast UV cure with secondary moisture cure.
  • Soft, flexible, low-modulus sealing material.
  • Excellent adhesion to plastics and metals.
  • Functional strength develops almost immediately after UV exposure.
  • Service temperature range from -40°C to +150°C.

Recommended Applications

  • Foam-in-place gasketing.
  • Plastic enclosure sealing.
  • Metal housing sealing.
  • Environmental protection seals.
  • Serviceable gasket applications.
Product Family

LOCTITE SI 5470

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White/pale yellow paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.03

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — Dual-cure foam gasket system
Chemical Type Acetoxy Silicone — Foamed silicone formulation
Appearance White / Pale Yellow Paste — Uncured material
Components One Component with Nitrogen Gas — Mechanically mixed
Primary Cure Ultraviolet Light — Rapid cure mechanism
Secondary Cure Moisture — Shadow-area curing
Temperature Range -40 to +150 °C Service range
Specific Gravity 1.03 — 25°C
Extrusion Rate 155 g/min 0.62 MPa, 25°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Tack-Free Time 15 seconds ASTM C679, 70 mW/cm² @ 365 nm
UV Depth of Cure 12 mm 60 sec @ 70 mW/cm²
Shore Hardness 54 Durometer OO ISO 868
Elongation at Break 163 % ISO 37
Tensile Strength 0.3 N/mm² ISO 37
Compression Set (20% Deflection) 21 % 22 h @ 25°C
Compression Set (30% Deflection) 20 % 22 h @ 25°C
Compression Set (40% Deflection) 19 % 22 h @ 25°C

Leading Brands Trust in Our Products and Services