LOCTITE® SI 5015 is a one-component acetoxy silicone RTV gasketing compound that cures at room temperature upon exposure to atmospheric moisture to form a tough, flexible silicone rubber gasket. The material provides excellent resistance to aging, weathering, vibration, and thermal cycling without hardening, shrinking, or cracking. It is designed for gasket replacement and gasket dressing applications and adheres to a wide variety of substrates. Typical automotive applications include valve covers, timing gear covers, differential covers, oil pans, transmission pans, water pumps, and thermostat housings.

Key Features & Benefits

  • Room-temperature vulcanizing (RTV) silicone gasket maker.
  • Provides tough, flexible silicone rubber seals.
  • Resists aging, weathering and thermal cycling.
  • Will not harden, shrink or crack during service.
  • Enhances load-bearing and shock-absorbing characteristics.
  • Safe for use with automotive oxygen sensors.
  • Adheres to a broad range of substrates.

Recommended Applications

  • Valve covers.
  • Timing gear covers.
  • Differential covers.
  • Oil pans and transmission pans.
  • Water pumps and thermostat housings.
  • Gasket replacement and gasket dressing applications.
Product Family

LOCTITE SI 5015

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Blue paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.04

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — RTV gasketing compound
Chemical Type Acetoxy Silicone — One-component system
Appearance Blue Paste — Uncured material
Specific Gravity 1.04 — 25°C
Odor Acetic Acid — Typical
Extrusion Rate ≥250 g/min 0.62 MPa, 25°C, 1/8 in nozzle
Flow ≤7.5 mm ISO 7390
Tack-Free Time ≤60 minutes 25°C / 50% RH
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Operating Temperature Range -54 to +204 °C Typical service range
Shore Hardness >25 Shore A ISO 868, cured 7 days
Flexibility Excellent — Absorbs vibration and shock loads
Thermal Cycling Resistance Excellent — Does not crack or shrink
Weathering Resistance Excellent — Outdoor durability
Motor Oil Resistance Retains Properties — Automotive fluid exposure
Transmission Fluid Resistance Retains Properties — Automotive fluid exposure
Antifreeze Resistance Retains Properties — Coolant exposure