LOCTITE SF768

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE SF768

Main features

  • Cyanoacrylate Residue Removal
  • Very-Low-Viscosity Solvent Cleaner
  • Surface Cleaning and Debonding

Product Description

LOCTITE® SF 768™ is a solvent-based cleaner formulated specifically for the removal of cured cyanoacrylate adhesives and for debonding components assembled with instant adhesives. The low-viscosity blend of nitromethane and hydrocarbon solvents penetrates cured adhesive deposits, allowing adhesive residues to be softened and removed from surfaces. It is suitable for maintenance, rework, and cleaning applications involving cured cyanoacrylate contamination. Based on the uploaded datasheet image.

Key Features & Benefits

  • Specialized solvent cleaner for cured cyanoacrylate removal.
  • Designed to debond cyanoacrylate-assembled parts.
  • Very low viscosity for rapid penetration.
  • Suitable for surface cleaning and adhesive residue removal.
  • Can soften cured adhesive in minutes to hours depending on thickness.
  • Effective on thin films, thick beads and assembled components.

Recommended Applications

  • Removal of cured cyanoacrylate adhesive residues.
  • Debonding assemblies bonded with instant adhesives.
  • Cleaning contaminated surfaces.
  • Maintenance and repair operations.
  • Rework of cyanoacrylate-bonded components.
Product Family

LOCTITE SF768

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear to yellow
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1.5 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Solvent Cleaner — Cyanoacrylate adhesive remover
Chemical Type Nitromethane / Hydrocarbon — Solvent blend
Appearance Clear to Yellow — As supplied
Viscosity Very Low — Product characteristic
Specific Gravity 1.1 — 25°C
Viscosity 1.5 mPa·s (cP) 20°C
Cure Not Applicable — Cleaner product
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Thin Adhesive Layer Removal Wipes Off Easily — Using SF 768 soaked cloth or tissue
Thick Bead Removal Time 15 to 30 minutes May require reapplication
Bonded Assembly Soak Time Several Hours — For debonding assembled parts
Adhesive Softening Rate Several Minutes to Several Hours — Depends on adhesive quantity
Cyanoacrylate Debonding Effective — For cured CA adhesive assemblies
Cleaning Function Surface Residue Removal — Maintenance and rework operations
Reapplication Requirement May Be Required — For thick adhesive deposits

Leading Brands Trust in Our Products and Services