LOCTITE SF7452

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE SF7452

Main features

  • Cyanoacrylate Adhesive Cure Accelerator
  • Fast Assembly Fixturing
  • Low-Viscosity Bonding Flow

Product Description

LOCTITE® SF 7452 is a cyanoacrylate adhesive activator designed to significantly increase the cure speed and fixture speed of LOCTITE® instant adhesives. The activator can be applied either before or after adhesive application and is particularly effective for rapid fixturing on production assemblies. It is commonly used in electronics and component assembly applications, including securing wires and coils to PCBs, mounting stand-offs, edge guides, and board stiffeners.

Key Features & Benefits

  • Cyanoacrylate adhesive cure accelerator.
  • Can be used as a pre- or post-applied activator.
  • Provides rapid fixture development.
  • Very low viscosity for easy application.
  • Suitable for automated and production assembly operations.
  • Qualified to Commercial Item Description A-A-3097.
  • Compatible with LOCTITE® cyanoacrylate adhesives.

Recommended Applications

  • Securing wires and coils to PCBs.
  • Tamper-proofing adjustable components.
  • Mounting stand-offs and edge guides.
  • Board stiffener installation.
  • Accelerating fixture speed of cyanoacrylate assemblies.
Product Family

LOCTITE SF7452

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent to slightly hazy liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.79
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
0.4 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Activator for Cyanoacrylate — CA adhesive accelerator
Chemical Type Organic Disulphide — Active ingredient
Solvent Acetone — Carrier solvent
Appearance Transparent to Slightly Hazy Liquid — As supplied
Specific Gravity 0.79 — 23°C
Viscosity 0.4 mPa·s (cP) 25°C
Drying Time 30 seconds 23°C
On-Part Life 5 minutes Typical
Approval A-A-3097 — Commercial Item Description
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Fixture Time 10 seconds ISO 4587, Steel (grit blasted), LOCTITE® 495, two-side activation
Application Method Pre- or Post-Activation — Flexible manufacturing process
Activator Open Time 5 minutes Maximum recommended time before bonding
Surface Activation Spray, Brush or Dip — Application options
Evaporation Requirement Required Before Bonding — Prevents solvent entrapment
Rapid Fixture Performance Excellent — For cyanoacrylate adhesive assemblies
PCB Assembly Suitability Suitable — Wire and coil securing applications
Tamper-Proofing Applications Recommended — Adjustable component locking