LOCTITE LB8801

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8801

Main features

  • Non-Curing Silicone Grease Formulation
  • High and Low Temperature Stability
  • Metal and Plastic Compatibility

Product Description

LOCTITE® LB 8801 is a non-curing silicone grease lubricant supplied in aerosol format for sealing, lubricating, protecting, waterproofing, and electrically insulating metal, rubber, and plastic components. The product provides excellent resistance to water, steam, alcohols, mineral oils, and vegetable oils while maintaining performance across a broad temperature range. It is commonly used as a moisture barrier for electrical contacts, a lubricant for rubber and plastic parts, and a protective coating against water infiltration and electrical arcing.

Key Features & Benefits

  • Non-curing silicone grease formulation.
  • Excellent water and steam resistance.
  • High and low temperature stability.
  • Lubricates, seals and waterproofs components.
  • Provides electrical insulation properties.
  • Protects electrical connections against water intrusion and arcing.
  • Compatible with metal, rubber and plastic substrates.

Recommended Applications

  • Electrical contact protection.
  • Moisture barriers for connectors and terminals.
  • Lubrication of rubber and plastic components.
  • Mold release applications.
  • Waterproofing and sealing assemblies.
  • Electrical insulators and mounting systems.
Product Family

LOCTITE LB8801

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Translucent
Density (g)
8.3 g/cm3
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.01

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone Grease — Non-curing lubricant
Appearance Translucent — As supplied
Density 8.3 lb/gal 25°C
Specific Gravity 1.01 — 25°C
Penetration (Unworked) 250 - 400 0.1 mm ISO 2137
Weight per Gallon 8.0 - 8.4 lb/gal Typical
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Dielectric Strength 22.8 kV/mm IEC 60243-1
Dielectric Constant 2.33 — 1 kHz, IEC 60250
Dissipation Factor 0.0045 — 1 kHz, IEC 60250
Dielectric Constant 2.37 — 1 MHz, IEC 60250
Dissipation Factor 0.001 — 1 MHz, IEC 60250
Water Resistance Excellent — Water and steam exposure
Fluid Resistance Excellent — Water-based fluids, alcohols, mineral & vegetable oils