LOCTITE LB8150

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8150

Main features

  • Graphite/Aluminum Anti-Seize Lubricants
  • Extreme-Pressure Additive Package
  • MIL-PRF-907-H Requirement Compliance

Product Description

LOCTITE® LB 8150™ is a high-temperature anti-seize lubricant formulated with mineral oil, lithium soap, graphite, aluminum and extreme-pressure additives to protect threaded assemblies exposed to severe thermal conditions. The non-curing compound prevents seizure, galling, corrosion, and jamming of threaded components operating at temperatures up to 900°C. It is particularly suitable for exhaust systems, burners, and industrial equipment where reliable assembly and future disassembly are required.

Key Features & Benefits

  • High-temperature anti-seize formulation.
  • Protects threaded connections from seizing and corrosion.
  • Contains graphite and aluminum lubricating solids.
  • Extreme pressure additive technology.
  • Suitable for service temperatures up to 900°C.
  • Prevents jamming in high-temperature assemblies.
  • Tested to MIL-PRF-907-H requirements.

Recommended Applications

  • Exhaust systems of combustion engines.
  • Oil and gas burner fittings.
  • High-temperature threaded fasteners.
  • Industrial furnace and thermal processing equipment.
  • Maintenance applications requiring future disassembly.
Product Family

LOCTITE LB8150

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Grey
Density (g)
0.9 g/cm3

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Anti-Seize — Non-curing lubricant
Chemical Type Mineral Oil, Lithium Soap, Graphite, Aluminum & EP Additives — High temperature formula
Appearance Grey — As supplied
Density 0.9 g/mL ISO 2811-1 @ 25°C
NLGI Consistency 1 Class ISO 6743-99
Worked Penetration 310 - 340 0.1 mm ISO 2137, 60 strokes @ 25°C
MIL Specification MIL-PRF-907-H — Tested to specification requirements
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Operating Temperature Range -30 to +900 °C Typical service range
Peak Temperature 900 °C Maximum rated temperature
4-Ball Weld Load 4,400 N ASTM D2596
Weld Scar Diameter <4.0 mm ASTM D2596 @ 4,400 N
Wear Scar 0.95 mm 1 hour / 400 N test
Copper Corrosion 1b Rating ISO 2160, 3 h @ 100°C
Seizure Prevention Excellent — High-temperature threaded assemblies
Corrosion Protection Excellent — Prevents thread seizure and galling