LOCTITE LB8036

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8036

Main features

  • Non-Metallic Grease Material
  • High-Lubricity Thread Assembly
  • 29C to 1093C Service Temperature

Product Description

LOCTITE® LB 8036 White High Temperature Anti-Seize is a premium non-metallic anti-seize compound designed to prevent galling, seizing, and corrosion of threaded and mated metal components exposed to extreme temperatures and harsh environments. The aluminum complex based formulation provides excellent lubricity, superior water resistance, and protection against galvanic corrosion while allowing easier assembly and disassembly of components. The product is compatible with a wide variety of metals including copper, brass, cast iron, steel, stainless steel, and other alloys.

Key Features & Benefits

  • Non-metallic anti-seize formulation.
  • Typical service temperature range from -29°C to 1093°C.
  • Excellent lubricity for threaded assemblies.
  • Superior water washout resistance.
  • Superior water spray resistance.
  • Prevents galvanic corrosion.
  • Permits easy assembly and disassembly of metal parts.

Recommended Applications

  • Bolts, screws, studs and nuts.
  • Pipe joints, shafts and bushings.
  • Splines, chains and cables.
  • Crane assemblies and industrial ovens.
  • Power plant turbine studs and inlet heater assemblies.
  • Coal crushers, pulp and paper mills.
  • Water and wastewater treatment facilities.
Product Family

LOCTITE LB8036

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Anti-Seize Compound — Non-metallic formulation
Chemical Type Aluminum Complex — Base thickener system
Appearance White Paste — As supplied
Specific Gravity 1.10 — Typical value
Unworked Penetration 320 mm/10 ASTM D217
Worked Penetration (60 strokes) 322 mm/10 ASTM D217
Flash Point >200 °F TCC
Weight per Gallon 9.2 lb/gal Typical value
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Service Temperature Range -29 to +1093 °C Typical operating range
Lubricity K-Factor 0.164 — 5,000 lb clamp load
Lubricity K-Factor 0.166 — 6,000 lb clamp load
Water Washout 0.33 % ASTM D1264
Copper Corrosion No Visible Change — ASTM D130-94
Oil Separation 0.94 % FTM 791 Method 321.3
Salt Fog Corrosion Resistance No Visible Change — ASTM B117
Galvanic Corrosion Protection Excellent — Multi-metal assemblies
Water Spray Resistance Superior — Wet environments

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers