LOCTITE LB8023

Main features

  • Calcium-Sulfonate Grease Formulation
  • High-Lubricity Thread Assembly
  • Galvanic Corrosion Prevention

Product Description

LOCTITE® LB 8023™ Marine Grade Anti-Seize is a calcium sulfonate-based anti-seize lubricant specifically formulated to protect assemblies exposed to fresh water, salt water, and high humidity environments. The non-curing paste provides exceptional lubricity, prevents galvanic corrosion, and offers superior resistance to water spray and water washout. It is ideal for marine, water treatment, and industrial maintenance applications requiring long-term corrosion protection and ease of disassembly under severe service conditions.

Key Features & Benefits

  • Calcium sulfonate-based anti-seize technology.
  • Excellent lubricity for threaded assemblies.
  • Prevents galvanic corrosion.
  • Superior resistance to water spray exposure.
  • Outstanding water washout resistance.
  • Protects against galling and seizing.
  • Suitable for marine and high-humidity environments.

Recommended Applications

  • Marine bolts, screws, studs and nuts.
  • Pipe joints, shafts, bushings and splines.
  • Chains and wire cables.
  • Water pump gaskets and flange dressing.
  • Pulp and paper mills.
  • Water and wastewater treatment facilities.
Product Family

LOCTITE LB8023

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Smooth, dark gray to black paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.25

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Calcium Sulfonate Based — Marine-grade anti-seize lubricant
Appearance Smooth Dark Gray to Black Paste — Non-curing paste
Specific Gravity 1.25 — 25°C
Penetration 300 - 380 0.1 mm ISO 2137
Weight per Gallon 1.2 - 1.36 kg/L Typical density range
Water Resistance 0.0 % ASTM D1264
Oil Separation 0.21 % wt. loss ASTM D6184 @ 25°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Operating Temperature Range -29 to +1315 °C Service temperature range
Torque Coefficient (K Factor) 0.18 — 3/8 × 16 steel nuts and bolts
Copper Corrosion No Visible Change — ISO 2160
Water Washout 0.0 % ASTM D1264
Galling & Seizing Test No Visible Change — PRF-907E Method 4.5.2.1
Salt Fog Corrosion Resistance No Visible Change — ASTM B117
Galvanic Corrosion Protection Excellent — Marine assemblies
Water Spray Resistance Superior — High humidity and marine environments