LOCTITE LB8017

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE LB8017 LOCTITE LB8017 LOCTITE LB8017 LOCTITE LB8017

Main features

  • Multi-Method Dry-Film Application
  • 400 deg C Sliding Service
  • 1315 deg C Anti-Seize Range

Product Description

LOCTITE LB 8017 is a one-component molybdenum-disulfide solid-film lubricant for lubrication and anti-seize service. The black coating can be brushed, dipped or sprayed onto clean metal surfaces, dries in 60 minutes at 25 deg C, and does not require mixing. A typical dry-film coverage of 55.7 m^2 per 4.5 kg is reported at 0.018 mm thickness. The applied film supports continuous sliding-friction service from -29 to 400 deg C and anti-seize use from -29 to 1315 deg C. Heat curing at 204 to 260 deg C thermosets the film for increased resistance to fluids and solvents.

Key features

  • Multi-method application: The lubricant can be brushed, dipped or sprayed directly onto clean metal surfaces.
  • High-temperature dry film: The applied film supports continuous sliding service to 400 deg C and anti-seize service to 1315 deg C.
  • Thermoset fluid resistance: Heat schedules from 204 to 260 deg C convert the film to a fluid- and solvent-resistant state.

Applications

Applications include threaded lubrication, dry bearings, slides, guides, pins, conveyor chains, exposed gears, press fits and selected aerospace or electrical mechanisms.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black
Chemistry Type
Molybdenum-disulfide based
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
One component
Solids
48 to 53 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.3
Physical Properties
Drying Time
1 hours

Additional Information

Technical properties

As-supplied properties

Typical as-supplied properties and dry-film coverage.

Property Value Unit Method / condition
AppearanceBlackAs supplied
Specific gravity1.3At 25 deg C
Density1.29g/mlAt 25 deg C
Solids / nonvolatile content48 to 53%As supplied
Weight per gallon10.5 to 11.1lb/galAs supplied
Dry-film coverage55.7m^2 per 4.5 kgAt 0.018 mm dry-film thickness
Technical properties

After-application / in-service properties

After-application and in-service behavior under the stated film condition and test configuration.

Property Value Unit Method / condition
Continuous sliding-friction range-29 to 400deg CApplied solid-film lubricant
Anti-seize operating range-29 to 1315deg CApplied anti-seize film
Torque coefficient0.06 to 0.1212.7 mm grade 8 steel bolts with grade 5 nuts
Unlubricated torque coefficient0.27Same bolt-and-nut configuration, solvent cleaned
Air-dried film fluid behaviorWithstands water and water solutionsMay soften or dissolve in organic solvents and oils
Oven-cured film fluid behaviorDoes not dissolve in most solvents and fluidsAfter a thermoset cure at 204 to 260 deg C

Leading Brands Trust in Our Products and Services