LOCTITE LB8009

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8009

Main features

  • Steel Compatibility Paste Material
  • Improved Clamp Load Consistency
  • Non-Curing Assembly Formulation

Product Description

LOCTITE® LB 8009® Heavy Duty Anti-Seize is a premium graphite and calcium fluoride based anti-seize lubricant formulated to protect threaded assemblies and metal components exposed to extreme temperatures and harsh industrial environments. The metal-free formulation contains no lead, copper, sulfur, or related compounds, making it compatible with stainless steel and nickel alloys. It provides long-term lubrication, prevents galling and seizure, and facilitates disassembly of components operating from -29°C to +1315°C.

Key Features & Benefits

  • Graphite and calcium fluoride anti-seize formulation.
  • Free from lead, copper, sulfur and free metals.
  • Compatible with stainless steel and nickel alloys.
  • Protects against galling, seizing and corrosion.
  • Provides improved clamp load consistency.
  • Suitable for extremely high temperature applications.
  • Non-curing lubricant paste.

Recommended Applications

  • Bolts, screws, studs and nuts.
  • Pipe joints, plugs and bushings.
  • Extrusion and forming dies.
  • Heat exchangers and shear blades.
  • Metal bending and mechanical packings.
  • Chemical plants, refineries, power plants and steel mills.
  • Marine, aerospace and industrial maintenance applications.
Product Family

LOCTITE LB8009

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Grey paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.15

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Anti-Seize Lubricant — Graphite / calcium fluoride formulation
Appearance Grey Paste — Non-curing
Specific Gravity 1.15 — 25°C
Penetration 270 - 370 0.1 mm ISO 2137
Weight per Gallon 9.6 - 10.6 lb/gal Typical
Metal Content None — Lead, copper and sulfur free
Compatibility Stainless Steel & Nickel Alloys — Suitable for corrosion-sensitive assemblies
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Operating Temperature Range -29 to +1315 °C Continuous service range
Torque Coefficient (K Factor) 0.16 — Lubricated 12.7 mm grade 8 steel bolt
Torque Coefficient (K Factor) 0.27 — Unlubricated solvent-cleaned bolt
Clamp Load Efficiency Improved — Provides higher clamp load at equivalent torque
Clamp Load Uniformity Enhanced — More consistent bolt preload distribution
Corrosion Protection Excellent — Protects threaded assemblies from seizure
Galling Resistance Excellent — For stainless steel and alloy assemblies
Disassembly Protection Prevents Seizing — Facilitates future maintenance

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers