LOCTITE EIF1000

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EIF1000

Main features

  • Phase-Change Surface Conformability
  • Kapton-Based Electrical Isolation
  • Residue-Free Pad Replacement

Product Description

LOCTITE EIF 1000 is an amber, electrically isolating phase-change thermal interface film supplied as a dry compound on a Kapton MT substrate. At approximately 60 deg C, the compound becomes thixotropic and conforms to mating surface features, helping expel interface air while the Kapton layer provides electrical isolation. Available as die-cut pads, multi-pad sheets or continuous rolls, the material supports repeatable installation between heat-generating components and heat sinks or chassis. It operates up to 150 deg C and can be removed without leaving foreign residue, allowing a replacement pad to be installed without further cleaning.

Key features

  • Phase-change conformability: The compound flows at approximately 60 deg C to conform to interface surfaces.
  • Kapton-based isolation: Electrical isolation is provided by the Kapton MT substrate.
  • Reworkable pad formats: Die-cut pads, sheets and rolls can be removed without foreign residue.

Applications

Applications include thermal interfaces between non-isolated heat-dissipating components and heat sinks or chassis.

Technical Specifications

General Properties
Chemistry Type
expanding modified epoxy film
Color
The color
Amber
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
5100 µm
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
7600 μm
Thermal Properties
Operating Temperature
up to 150ºC °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.45 W/m.K
Thermal Impedance
1.29 °C·cm²/W
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
177-196 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1×10^14 Ohms⋅cm
Thermal Properties
Phase Change Temperatur
60 °C

Additional Information

Technical properties

As-supplied properties

Construction, available formats and thickness options before installation.

Property Value Unit Method / condition
AppearanceAmberAs supplied
ConstructionDry phase-change compound on Kapton MTElectrically isolating substrate
Available formatsSingle die-cut pads, multi-pad sheets, continuous rollsCustom parts also available
KA thickness0.051 substrate; 0.076 totalmmKA construction
KB thickness0.025 substrate; 0.051 totalmmKB construction
K3 thickness0.076 substrate; 0.102 totalmmK3 construction
Phase-change temperature60deg CCompound becomes thixotropic above phase change
Optimal storageBelow 40deg CUnopened container in a dry location
Technical properties

Final-state properties

Installed thermal and electrical values; thermal impedance is variant-specific at 80 psi.

Property Value Unit Method / condition
KA thermal impedance1.29deg C cm^2/WASTM D5470 at 80 psi; 0.076 mm total thickness
KB thermal impedance0.776deg C cm^2/WASTM D5470 at 80 psi; 0.051 mm total thickness
K3 thermal impedance1.88deg C cm^2/WASTM D5470 at 80 psi; 0.102 mm total thickness
Thermal conductivity0.45W/(m K)Reported for KA, KB and K3 constructions
Volume resistivity1 x 10^14ohm-cmKapton MT substrate data
Dielectric strength4,500 to 5,000VAC/milASTM D149-91; Kapton MT substrate data
Dielectric constant4.2Kapton MT substrate data
Cut-through resistance18.1kgDuPont test method

Leading Brands Trust in Our Products and Services