LOCTITE EF562S

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EF562S LOCTITE EF562S

Main features

  • Non-Asbestos Honeycomb Bonding
  • Roll-or-Sheet Layup Flexibility
  • Expanding Core Reinforcement

Product Description

LOCTITE EF 562S AERO is a non-asbestos, unsupported modified epoxy foaming film adhesive for sealing, splicing and reinforcing honeycomb materials. Supplied in roll or sheet form, the film is cut and positioned during lay-up before heat cure. Its expanding behavior fills localized honeycomb details, while the unsupported construction allows direct placement without a carrier fabric. The product supports aerospace honeycomb fabrication processes that specify EF 562S and its specified cure and expansion conditions.

Key features

  • Non-asbestos formulation: The modified epoxy foaming adhesive is supplied without asbestos reinforcement.
  • Roll or sheet format: The unsupported film is available in forms suited to cutting and lay-up.
  • Expanding honeycomb reinforcement: Heat-cure expansion supports sealing, splicing and reinforcing honeycomb details.

Applications

Applications include sealing, splicing and reinforcing aerospace honeycomb materials.

Product Family

LOCTITE EF562S

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Unsupported expandable epoxy film adhesive
Color
The color
Amber
Density (g)
0.51 g/cm3
Physical Properties
Volatiles
0.14 %

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers