LOCTITE EF562

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE EF562

Main features

  • Foaming Epoxy Film Adhesive
  • Uniform Cell Structure
  • Dual-Cure Bonding Processing

Product Description

LOCTITE® EF 562 AERO (formerly Hysol® MA 562) is a foaming epoxy film adhesive designed for honeycomb core splicing, sealing, and reinforcement applications in aerospace composite structures. The unsupported expandable adhesive cures at either 250°F (121°C) or 350°F (177°C) and develops a uniform closed-cell structure that helps reduce moisture ingress into splice areas. Its low exotherm, excellent slump resistance, and dual-cure capability make it particularly suitable for thick splice sections and co-cure manufacturing processes.

Key Features & Benefits

  • Foaming epoxy film adhesive for aerospace honeycomb structures.
  • Uniform cell structure reduces moisture ingress into splice areas.
  • Dual cure schedules at 250°F (121°C) or 350°F (177°C).
  • Excellent slump resistance during processing.
  • Low exotherm suitable for thick bond lines and co-cure assemblies.
  • Asbestos-free formulation.
  • Qualified to numerous aerospace industry specifications.

Recommended Applications

  • Honeycomb core splicing.
  • Honeycomb edge closeouts.
  • Structural reinforcement of composite core panels.
  • Sealing honeycomb core sections.
  • Co-cure composite panel manufacturing.
Product Family

LOCTITE EF562

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Yellow
Density (g)
0.4 g/cm3

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Expandable Epoxy Film Adhesive — Unsupported film adhesive
Appearance Yellow — Film adhesive
Volatile Content <1 % Typical
Available Thickness 0.050 / 0.100 in 1.3 / 2.5 mm
Form 1 × 2 Sheets ft Approx. 0.3 × 0.6 m
Slump <0.125 in <3.18 mm
Expansion 2 to 3.5× — Original uncured thickness
Exotherm <550 °F 0.200 in thickness
Cured Density 25 to 35 lb/ft³ 0.40 to 0.56 g/cc
Shelf Life 6 months ≤ -18°C storage
Out Time 10 days @ 32°C / 20 days @ 24°C — Maximum exposure time
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Service Temperature Range -55 to +177 °C Continuous service
Cure Schedule 60 min @ 121°C or 177°C — 5-10°F/min heat-up rate
Tube Shear Strength 1200 psi 24°C, cured 121°C
Tube Shear Strength 1150 psi 24°C, cured 177°C
Water Boil Retention 1095 psi 3-day water boil exposure
Skydrol Resistance 1085 psi 7 days @ 68°C
Salt Spray Retention 780 psi 30-day exposure
Flexural Strength 830 psi 24°C, cured 121°C
Flexural Strength 770 psi 24°C, cured 177°C
High Temperature Flexural Strength 540 psi 177°C test temperature

Leading Brands Trust in Our Products and Services