LOCTITE EF557

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EF557 LOCTITE EF557

Main features

  • Expanding Honeycomb Gap Filling
  • Film-Based Splice Reinforcement
  • Dual-Temperature Cure Flexibility

Product Description

LOCTITE EF 557 AERO is an expandable modified epoxy film adhesive for sealing, splicing and reinforcing aerospace honeycomb materials. Supplied as a preformed foaming film, it expands during the stated heat-cure cycle to fill and bridge honeycomb details without liquid component mixing. The film supports localized core reinforcement, edge sealing and splice work where a controlled lay-up format is preferred. Dual-temperature cure options provide process flexibility for compatible honeycomb assemblies while retaining the required cure and expansion conditions for the selected construction.

Key features

  • Expandable film fill: The modified epoxy film expands during heat cure to fill honeycomb details.
  • Honeycomb assembly functions: The product supports sealing, splicing and reinforcement of honeycomb materials.
  • Dual-temperature cure options: Two heat-cure routes are identified for the supplied film.

Applications

Applications include sealing, splicing and reinforcing aerospace honeycomb materials.

Technical Specifications

General Properties
Chemistry Type
modified epoxy foaming adhesive
Color
The color
Black
Density (g)
0.51 g/cm3
Physical Properties
Volatiles
0.14 %