LOCTITE EDAG 423SS

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE EDAG 423SS

Main features

  • Graphite-Filled Conductive Ink
  • Low-Voltage Circuit Applications
  • Broad Screen-Printing Equipment Compatibility

Product Description

LOCTITE® EDAG 423SS E&C is a conductive, screen-printable graphite ink formulated with finely divided graphite particles dispersed in a thermoplastic resin system. The material is designed for printing low-voltage circuitry on polyester film substrates and is widely used in membrane touch switches, keyboards, printed resistors, flexible circuits, heating elements, and electrostatic discharge (ESD) protection applications. The ink provides excellent adhesion to polyester films, flexible processing conditions, and compatibility with standard screen-printing equipment.

Key Features & Benefits

  • Graphite-filled conductive screen-printable ink.
  • Designed for low-voltage printed circuitry applications.
  • Compatible with all types of screen-printing equipment.
  • Non-critical, low-temperature drying process.
  • Excellent screen residence time during production.
  • Excellent adhesion to polyester film substrates.
  • Suitable for ESD and conductive circuit applications.

Recommended Applications

  • Membrane touch switches.
  • Printed resistors and conductive tracks.
  • Membrane keyboards.
  • Heating elements.
  • Flexible printed circuits.
  • Electrostatic discharge (ESD) protection layers.
Product Family

LOCTITE EDAG 423SS

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Dark gray
Density (g)
1.1 g/cm3
Solids
36 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
78 °C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers