LOCTITE ECCOBOND EO 1061

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ECCOBOND EO1061

Main features

  • Extended Pot-Life Processing
  • Stable-Viscosity Dispensing Control
  • One-Part Heat-Cure Encapsulation

Product Description

LOCTITE® ECCOBOND EO1061 is a black, one-component, heat-cure epoxy encapsulant for chip-on-board assemblies and low-profile electronic devices. The medium-flow material contains 61.3 wt% filler and has typical viscosities of 50,000 mPa·s at 2 rpm and 32,500 mPa·s at 20 rpm at 25°C. Its viscosity stability at 25°C supports controlled shot sizing with conventional time/pressure dispensing equipment. A recommended cure of 3 hours at 140°C produces a cured glass transition temperature of 125°C. The product is designed for 1,000 hours of temperature/humidity/bias testing and thermal cycling up to 125°C. Because it is not thixotropic, a physical flow barrier is required during encapsulation.

Key features

  • Stable dispensing viscosity: Viscosity stability at 25°C supports controlled shot sizing with conventional time/pressure equipment.
  • Extended pot life: Typical pot life is 25 days at 25°C for a 200 g mass.
  • High-temperature cured profile: The cured material has a typical Tg of 125°C and CTE below Tg of 40 ppm/°C from 40 to 120°C.

Applications / Suitable for

  • Chip-on-board encapsulation
  • Low-profile electronic devices
Product Family

LOCTITE ECCOBOND EO 1061

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
600 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.78

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured properties and processing parameters. Values are reference data and are not guaranteed product specifications.

Property Value Unit Method / condition
Filler content 61.3 wt% As supplied
Specific gravity 1.78 — 25°C
Viscosity 50,000 mPa·s Brookfield RVF, spindle 6, 2 rpm, 25°C
Viscosity 32,500 mPa·s Brookfield RVF, spindle 6, 20 rpm, 25°C
Pot life 25 days 25°C; 200 g mass
Gel time 13 min 121°C
Recommended cure 3 h 140°C; curing below 125°C is not recommended
Optimal storage temperature −40 °C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Typical cured-material properties. Values are reference data and should not be treated as guaranteed design specifications.

Property Value Unit Method / condition
Coefficient of thermal expansion 40 ppm/°C Below Tg; 40 to 120°C
Glass transition temperature 125 °C Cured material
Linear shrinkage 1.07 % Cured material
Flexural strength 64.8 N/mm² Equivalent source value: 9,400 psi
Dielectric constant / dissipation factor 4.97 / 0.0083 — IEC 60250; 25°C; 1 kHz
Volume resistivity 1.9 × 1014 Ω·cm IEC 60093
Surface resistivity 2.0 × 1014 Ω IEC 60093